AISI 201 304 316 marinated asye pur tiyo soude

AISI 201 304 316 marinated asye pur tiyo soude

Klas ekivalan: 201 / 1.4372; 304 / 1.4301; 316 / 1.4401
Estanda: ASTM A312/ASTM A358/ASTM A269/EN 10217-7
Kalite soude: TIG soude / ERW / segondè-frekans soude
Dyamèt Eksteryè (OD): 6-630 mm; pi gwo gwosè disponib sou demann
Epesè miray: 0.5-30 mm; Customized dapre OD ak estanda
Longè: 5.8 m / 6 m / 11.8 m / 12 m; koupe-a-longè ki disponib
Fini andigman: marinated / asid marinated / marinated & passive
Tretman chalè: Solisyon rkwit / Kòm soude
Tiyo Fin: Plain Fen / Bizote Fen / Threaded Fen
Tretman soude: Weld chaplèt retire / soude & marinated / polisaj soude entèn ki disponib
Sètifika Materyèl: EN 10204 3.1 / 3.2 MTC
Marking: Klas, Gwosè, No Chalè, Estanda, Manifakti ak Pakèt No.
Anbalaj: bouchon plastik + papye ki enpèmeyab + PVC / PE fim + pakèt asye
Voye rechèch
Chat kounye a

Si w ap achte tiyo asye pur marinated soude nan klas AISI 201, 304, oswa 316 pou pwodui chimik, manje ak bwason, tretman dlo, achitekti, maren, oswa aplikasyon jeneral endistriyèl, kle a se nan chwazi bon klas la, epesè miray la, fini sifas, ak nivo enspeksyon ki baze sou anviwònman opere ou. Gnee founiti tiyo asye pur soude nan 201, 304, 316, 304L, ak 316L, ki kouvri dyamèt ekstèn soti nan apeprè 1/2 pous a 24 pous ak epesè miray soti nan 0.8 a 20 mm. Pwodwi yo vini konplè ak EN 10204 3.1 Sètifika Tès Materyèl (MTC) ak rapò Idantifikasyon Materyèl Pozitif (PMI), ki gen ladan tès idrostatik kòm estanda, ansanm ak sèvis enspeksyon radyografik (RT), ultrasons (UT), oswa likid penetran (PT).

304 Stainless Steel Pipe Material Certificate
Sètifika materyèl tiyo asye pur 304
316 Stainless Steel Pipe Material Certificate
Sètifika materyèl tiyo asye pur 316

An tèm de fabrikasyon, tiyo yo ka pwodwi lè l sèvi avèk pwosesis soude tankou ERW ak EFW, ak bon jan kalite risk tankou mank fizyon, enklizyon, ak oksid rezidyèl bese nan kontwòl fòm pèl soude, tretman sifas entèn / ekstèn, ak marinated. Sifas tipik Ra a se apeprè 1.2-2.5 μm, ki pa gen okenn teksti diferan direksyon woule vizib sou sifas la. Konsènan tretman sifas, sifas marinated / HFD yo tipikman cho-woule oswa soude, solisyon-annealed, ak marinated pou retire echèl, oksidasyon nan zòn ki afekte chalè a, ak kontaminan sifas yo, bay tiyo a yon aparans inifòm ajan-blan metalik.

Pwosesis Faktori
 

Resi asye band ak verifikasyon nimewo chalè → Koupe / preparasyon teren → Woulo fòme → Soude (ERW/TIG/Lazè) → Weld chaplèt echapman ak tretman → Dimansyon ak redresman → Solisyon annealing (soulajman estrès + restorasyon nan rezistans korozyon) → Pickling ak pasivasyon → Koupe-a-longè → Enspeksyon, tès ak sètifika MT, →

 AISI 201 Stainless Steel Pipe

Ki sa ki AISI 201 tiyo asye pur?

AISI 201 tiyo asye pur fè pati ekonomik austenitic asye pur, ak yon konpozisyon chimik tipik nan Cr 16-18%, Ni 3.5-5.5%, Mn 5.5-7.5%, ak C mwens pase oswa egal a 0.15%. Li diminye depans materyèl nan pi wo Mn ak pi ba kontni Ni, ki ofri yon avantaj pri siyifikatif sou 304. Li apwopriye pou kanal vantilasyon andedan kay la, tiyo dekoratif, pati estriktirèl mèb, ak anviwònman ki lejèman korozivite.

Ki sa ki AISI 304 tiyo asye pur?

AISI 304 tiyo asye pur se pi lajman itilize jeneral-purpose austenitic Nerjaveèi, ak Cr 18-20%, Ni 8-12%, C mwens pase oswa egal a 0.08%, ak yon PREN nan apeprè 18-20. 304 karakteristik bon fòmabilite, soudabilite, ak atmosferik apwopriye korozyon, rezistans manje ak presyon, fè li apwopriye pou korozyon, rezistans manje ak presyon. dekorasyon achitekti, ak estrikti jeneral endistriyèl.

 AISI 304 Stainless Steel Pipe
 AISI 316 Stainless Steel Pipe

Ki sa ki AISI 316 tiyo asye pur?

AISI 316 tiyo asye pur gen yon konpozisyon chimik nan Cr 16.5-18.5%, Ni 10-14%, Mo 2-3%, C mwens pase oswa egal a 0.08%, ak yon PREN nan apeprè 24-26. Anplis de sa nan Mo bay 316 siperyè rezistans korozyon lokal konpare ak 304 nan anviwònman ki gen Cl⁻, dlo lanmè, dlo ize klò, ak sèten kondansasyon asid; li apwopriye pou jeni maren, kanalizasyon medya chimik, sistèm refwadisman dlo lanmè, ak ekipman pharmaceutique.

201, 304, ak 316 Espesifikasyon Nerjaveèi

Pwodwi marinated & passive Nerjaveèi asye soude tiyo / tib (wonn)
Klas AISI 201, 304, 304L, 316, 316L (tou 321, 310S, 2205 sou demann)
Estanda ASTM A554, ASTM A312/A312M, ASTM A249, ASTM A269, EN 10217-7, JIS G3448, GB/T 12771
Pwosesis soude ERW (HF), TIG / GTAW, lazè soude
Tretman chalè Solisyon rkwit (klere rkwit oswa atmosfè rkwit) apre soude
Sifas fini marinated & pasivated (estanda); moulen, bwose, poli #180/#320/#400, glas ki disponib
Dyamèt ekstèn

6 mm - 610 mm (wonn) ·

kare 10×10 – 150×150 mm ·

rektangilè 20 × 10 - 200 × 100 mm

Epesè miray la 0.5 mm - 20 mm
Longè 3 m / 6 m estanda, oswa koupe nan longè koutim (jiska 12 m)
Sètifika EN 10204 3.1 Sètifika Tès Mill pou chak nimewo chalè (3.2 ak yon twazyèm pati temwen sou demann)
MOQ [ 1 × 20 pye veso ] pou gwosè estanda; ti lòd jijman aksepte pou echantiyon

 

Konpozisyon Chimik (Kondisyon Estanda % max, sof si sa endike otreman)

Eleman AISI 201 AISI 304 AISI 316
Kabòn (C) 0.15 0.08 0.08
Kwòm (Cr) 16.0 - 18.0 18.0 - 20.0 16.0 - 18.0
Nikèl (Ni) 3.5 - 5.5 8.0 - 10.5 10.0 - 14.0
Manganèz (Mn) 5.5 - 7.5 2.0 2.0
Molybdène (Mo) - - 2.0 - 3.0
Silisyòm (Si) 1.0 1.0 1.0
Fosfò (P) 0.06 0.045 0.045
Souf (S) 0.03 0.03 0.03

 

Pwopriyete mekanik (valè tipik)

Klas Fòs rupture (MPa) Fòs Sede (MPa) elongasyon (%) Dite (HB)
AISI 201 Pi gran pase oswa egal a 515 Pi gran pase oswa egal a 275 Pi gran pase oswa egal a 40 Mwens pase oswa egal a 217
AISI 304 Pi gran pase oswa egal a 515 Pi gran pase oswa egal a 205 Pi gran pase oswa egal a 40 Mwens pase oswa egal a 201
AISI 316 Pi gran pase oswa egal a 515 Pi gran pase oswa egal a 205 Pi gran pase oswa egal a 40 Mwens pase oswa egal a 217

 

Tolerans estanda dimansyon (ASTM A312)

Dimansyon Ranje aplikab Tolerans
Dyamèt deyò (OD) 1/8"-1-1/2" (10.3-48.3 mm) +0.40 / -0.80 mm
Dyamèt deyò (OD) 2"-4" (60.3-114.3 mm) +0.80 / -0.80 mm
Dyamèt deyò (OD) 5"-8" (141.3-219.1 mm) +1.20 / -1.20 mm
Epesè miray (WT) WT Mwens pase oswa egal a 2.5 mm +20% / -12.5%
Epesè miray (WT) WT > 2.5 mm +15% / -12.5%

 

201 vs. 304 vs. 316 Tiyo Nerjaveèi: Kijan pou w chwazi?

AISI 201/304/316 Pickled Nerjaveèi asye soude tiyo yo ka aplike nan vantilasyon achitekti ak tiyo echapman, tiyo pwosesis chimik ki ba-presyon, sistèm refwadisman dlo lanmè, liy transpò manje ak pharmaceutique, dekorasyon achitekti, ak jeneral kad estriktirèl endistriyèl.

Pou pwojè priyorite bidjè ak kondisyon korozivite twò grav, 201 ka konsidere; pou pifò anviwònman jeneral endistriyèl ak manje-klas, 304 ofri yon chwa ki pi ekilibre; ak pou kondisyon fonksyònman ki enplike klori, anviwònman maren, oswa pi gwo risk nan korozyon lokalize, 316 rekòmande.

Pou ede w chwazi tiyo ideyal la pou pwojè w la, èske w ka pataje:
Anviwònman opere (andedan, deyò, bò lanmè, oswa plant chimik)?
Ki sibstans oswa likid tiyo yo pral pote?

Kontakte kounye a

 

Tan livrezon

Pou egzekisyon pwojè, pwodwi yo ka fabrike an akò ak estanda aplikab tankou ASTM A312/ASME SA312, ASTM A358, ASTM A269, EN 10217-7, ak JIS G3459, pandan y ap satisfè kondisyon espesifik pwojè yo anba kòd tankou ASME B31.3 ak PED 2014/68/EU. Livrezon pou espesifikasyon ki estoke yo ka anjeneral ranje nan apeprè 2-3 semèn, tandiske espesifikasyon ki pa estoke oswa espesyal jeneralman mande pou apeprè 6-10 semèn; tan aktyèl yo depann de klas materyèl la, dimansyon, kantite, kondisyon tès yo, ak orè pwodiksyon an.

 

Kontwòl Kalite

Tès estanda gen ladan analiz konpozisyon chimik, enspeksyon dimansyon ak vizyèl, tès rupture, tès dite, tès plat, ak tès idrostatik. Tou depan de kondisyon pwojè yo, sèvis adisyonèl ki disponib, ki gen ladan 100% tès idrostatik, PMI (verifikasyon alyaj OES), ak tès ki pa destriktif (RT, UT, PT), osi byen ke kalkil PREN ak sèvis enspeksyon twazyèm pati soti nan SGS, BV, TÜV, oswa Intertek.

Flattening test
Tès aplati
Flaring test
Tès flaring
 
Hydrostatic testing
Tès idrostatik
Ultrasonic testing
Tès ultrasons
Tensile test
Tès tensile
Intergranular corrosion test
Tès korozyon entègranulèr

Anbalaj ekspòtasyon estanda

AISI 201/304/316 Pickled Nerjaveèi asye soude tiyo yo chaje ak bouchon plastik sou tou de bout, papye ki enpèmeyab ak fim PE / PVC pou pwoteje sifas la marinated kont imidite, reyur ak kontaminasyon. Tiyo yo byen pake ak espageti asye, ak chak pake byen make ak klas, OD, WT, longè, kantite ak nimewo chalè. Anbalaj ekspòtasyon Seaworthy se apwopriye pou veso ak transpò lanmè long distans.

Standard Export Packaging

Standard Export Packaging

 

FAQ

Ki sa ki marinated ak passive asye pur tiyo soude?
Li se yon tiyo soude asye pur ki te nan de tretman sifas apre soude. Pickling itilize yon beny asid melanje pou retire echèl oksid la ak koulè chalè ki te kreye pa soude a. Lè sa a, pasivasyon rebati kouch natirèl kwòm-oksid sou tout sifas la. Rezilta a se yon tiyo ki gen kouti soude se tankou korozyon ki reziste tankou metal debaz li yo, ak yon aparans pwòp, inifòm.

 

Ki diferans ki genyen ant 201, 304 ak 316 asye pur tiyo soude?
201 sèvi ak Manganèz olye de yon pati nan nikèl la, ki fè li pi bon mache nan twa a men pi piti a korozyon-rezistan - apwopriye pou itilizasyon sèk andedan kay la sèlman. 304 gen 8-12% nikèl epi li se klas estanda tout-wonn pou dlo ak sèvis manje. 316 ajoute 2-3% molybdène, ki ba li yon pi gwo endèks (2-24 REN). ≈ 18–19 pou 304), fè li chwa pou klori, dlo lanmè ak sèvis chimik.


Ki diferans ki genyen ant tiyo asye pur soude ak san pwoblèm?
Se tiyo san pwoblèm ki fòme apati yon billet solid ki pa gen okenn kouti soude; tiyo soude se woulo liv-fòme soti nan teren ak longitudinal soude. Pou pifò aplikasyon jeneral, manje-klas ak estriktirèl, yon tiyo soude byen rkwit ak marinated fè ekivalan a san pwoblèm nan yon pri siyifikativman pi ba. San pwoblèm nòmalman rezève pou sèvis trè wo-presyon oswa trè kritik. Di nou kondisyon sèvis yo epi n ap konseye kiyès ki vrèman nesesè.

 

Èske w ka bay yon Sètifika Tès Mill EN 10204 3.1?
Wi. Chak kagezon yo apwovizyone ak yon sètifika EN 10204 3.1 Depatman enspeksyon kalifye nou an te bay, ki ka trase nan nimewo chalè ki make sou chak tiyo. Si pwojè ou a mande pou verifikasyon endepandan, nou ka fè aranjman pou sètifikasyon 3.2 ak yon temwen twazyèm pati tankou SGS, BV oswa TÜV.

 

Ki fini sifas ki disponib?
marinated & pasivated se fini estanda nou an. Nou bay tou fini moulen, bwose / saten, poli #180, #320, #400, glas (600-800 gravye) ak fini electropolished. Fini seleksyon anjeneral swiv egzijans ijyèn oswa ayestetik aplikasyon an.

 

Èske ou aksepte enspeksyon twazyèm pati?
Wi, e nou ankouraje li. SGS, Bureau Veritas, TÜV, Intertek ak enspektè nominasyon kliyan yo tout akeyi nan nenpòt etap dakò - pandan pwodiksyon, anvan anbalaj oswa anvan chaje. Nou pral bay aksè, dokimantasyon ak enstalasyon tès ki nesesè yo.

 

Èske ou ka pwodwi gwosè koutim, longè ak klas?
Wi. Nou pwodwi dyamèt ekstèn ki pa estanda, epesè miray ak longè koupe nan desen, epi nou ka bay klas pi lwen pase seri estanda (321, 310S, 2205 duplex) sijè a yon kantite minimòm lòd. Voye nou desen an oswa spesifikasyon epi nou pral konfime posibilite ak tan plon.

Baj popilè: AISI 201 304 316 marinated Nerjaveèi asye soude tiyo, Lachin AISI 201 304 316 marinated Nerjaveèi asye soude tiyo manifaktirè, Swèd, faktori