Kouman pou mwen kalkile pwa a nan asye pur?

Pwa=Zòn Seksyon Transvèsal × Longè × Dansite. Kalkile transvèsal zòn fòm nan (π × d²/4 pou ba wonn; π × miray × (OD - mi) pou tiyo; lajè × epesè pou ba plat ak plak), miltipliye pa longè an mèt ak dansite klas la nan g/cm³ (7.93 pou 304/304L, 7.98 pou 310.0 kg), Lè sa a, jwenn pa 31 10.0. Pou dra kote lajè, longè ak epesè yo tout an mm, divize pa 1,000,000 pito.

 

Èske pwa kalkile a menm ak pwa aktyèl la?

Non. Pwa kalkile se pwa teyorik ki baze sou dimansyon nominal ak dansite nominal. Pwa aktyèl diferan akòz tolerans woule (± 5-10% sou epesè/dyamèt/miray), varyasyon konpozisyon chalè-a-chalè, retire materyèl sifas-fini (marinaj, polisaj), ak pratik tolerans mi-tiyo. Pifò moulen fakti sou pwa teyorik; toujou konfime baz pwa a ak founisè ou.

 

Ki sa ki dansite 304 asye pur?

304/304L asye pur gen yon dansite 7.93 g/cm³ (7930 kg/m³, 0.286 lb/in³). Menm valè a aplike a pi laj fanmi 300-seri - 201, 202, 301, 302, 303 ak 321 - pandan y ap 316/316L se yon ti kras pi lou nan 7.98 g/cm³.

 

Ki sa ki dansite 316 asye pur?

316/316L Nerjaveèi gen yon dansite 7.98 g/cm³ (7980 kg/m³, 0.288 lb/in³). Molybdène siplemantè a (2-3%) ki bay 316 rezistans siperyè pitting li tou fè li apeprè 0.6% pi lou pase 304.

 

Kouman pou mwen kalkile pwa a nan yon tiyo asye pur oswa tib?

Sèvi ak: Pwa (kg/m)=π × miray × (OD − miray) × ρ ÷ 1000 - OD ak mi an mm, ρ nan g/cm³. Yon tiyo 304, OD 21.3 × 2.77 mm, kidonk peze 3.14159 × 2.77 × 18.53 × 7.93 ÷ 1000 ≈ 1.28 kg/m. Sa a ap travay pou tou de tiyo san pwoblèm ak soude, tib wonn, ak tib presyon.

 

Konbyen yon fèy 4 × 8 nan asye pur 304 peze?

Yon fèy 4 pye × 8 pye (1219 × 2438 mm) 304 peze 23.6 kg (52.0 lb) pou chak 1 mm epesè. Valè komen: 2 mm → 47.2 kg (104 lb), 3 mm → 70.7 kg (156 lb), 6 mm → 141.5 kg (312 lb), ½″ (12.7 mm) → 299 kg (660 lb). Pou 316, miltipliye pa 1.006.

 

Dansite nominal nan klas Nerjaveèi komen

Klas / UNS Fanmi Dansite g/cm³ Dansite kg/m³ Dansite lb/in³
201, 202 (S20100, S20200) Austenitic 7.93 7930 0.286
301, 302, 303 (S30100, S30200, S30300) Austenitic 7.93 7930 0.286
304, 304L, 304H (S30400, S30403, S30409) Austenitic 7.93 7930 0.286
305 (S30500) Austenitic 8.00 8000 0.289
309, 309S (S30900, S30908) Austenitic 7.98 7980 0.288
310, 310S (S31000, S31008) Austenitic 7.98 7980 0.288
316, 316L, 316H (S31600, S31603, S31609) Austenitic 7.98 7980 0.288
316Ti (S31635) Austenitic 8.00 8000 0.289
317, 317L (S31700, S31703) Austenitic 8.00 8000 0.289
321 (S32100) Austenitic 7.93 7930 0.286
347 (S34700) Austenitic 8.00 8000 0.289
904L (N08904) Super austenitic 7.95 7950 0.287
409 (S40900) Feritik 7.70 7700 0.278
410 (S41000) Martensitic 7.70 7700 0.278
420 (S42000) Martensitic 7.70 7700 0.278
430 (S43000) Feritik 7.70 7700 0.278
434, 439 (S43400, S43035) Feritik 7.70 7700 0.278
440A / 440B / 440C (S44002–04) Martensitic 7.70 7700 0.278
446 (S44600) Feritik 7.50 7500 0.271
2205 Duplex (S32205 / S31803) Duplex 7.80 7800 0.282
2507 Super Duplex (S32750) Super duplex 7.80 7800 0.282
17-4PH (S17400) Presipitasyon-redi 7.80 7800 0.282
15-5PH (S15500) Presipitasyon-redi 7.80 7800 0.282

 

Pou kalkile pwa asye pur (plak, tiyo, oswa ba wonn) ki baze sou dimansyon espesifik ou ak inite (pous oswa milimèt), klike sou bouton ki anba a pou fè kalkil la.

kalkilatris