Kouman pou mwen jwenn klas ekivalan asye pur soti nan diferan peyi?
Pou jwenn klas asye pur ekivalan atravè diferan estanda nasyonal, sèvi ak yon tablo referans kwaze tankou sa ki nan paj sa a. Koresponn ak nòt ou konnen (pa egzanp, AISI 304) nan kolòn ki koresponn lan, epi li atravè ranje a pou jwenn ekivalan EN, JIS, GB, DIN, ak BS. Ou ka itilize ba rechèch la tou pou filtre pa nenpòt non klas, nimewo UNS, nimewo EN, oswa deziyasyon GB. Pou aplikasyon kritik, toujou konfime ekivalans ak dokiman ofisyèl ofisyèl yo (ASTM A240, EN 10088, JIS G4304, GB/T 4237, BS 970) epi konsilte avèk founisè materyèl ou a.
| AISI/ASTM | UNS | EN | DIN | JIS | GB (Lachin) | BS (UK) |
|---|---|---|---|---|---|---|
| 201 | S20100 |
1.4372 |
X12CrMnNiN17-7-5 | SUS201 |
12Cr17Mn6Ni5N |
- |
| 202 | S20200 |
1.4373 |
X12CrMnNiN18-9-6 | SUS202 |
12Cr18Mn9Ni5N |
284S16 |
| 301 | S30100 |
1.4310 |
X10CrNi18-8 | SUS301 |
12Cr17Ni7 |
301S21 |
| 302 | S30200 | 1.4300 | SUS302 |
12Cr18Ni9 |
302S25 | |
| 303 | S30300 |
1.4305 |
X10CrNiS18-9-9 | SUS303 |
Y12Cr18Ni9 |
303S31 |
| 304 | S30400 |
1.4301 |
X5CrNi18-10 | SUS304 |
06Cr19Ni10 |
304S15 |
| 304L | S30403 |
1.4307 |
X2CrNi18-10 | SUS304L |
022Cr19Ni10 |
304S11 |
| 304H | S30409 |
1.4948 |
X6CrNi18-10 | SUS304H |
07Cr19Ni10 |
304S51 |
| 305 | S30500 |
1.4303 |
X4CrNi18-12 | SUS305 |
06Cr18Ni12 |
305S19 |
| 309S | S30908 |
1.4828 |
X15CrNiSi20-12 | SUS309S |
06Cr23Ni13 |
309S24 |
| 310S | S31008 |
1.4845 |
X8CrNi25-21 | SUS310S |
06Cr25Ni20 |
310S24 |
| 316 | S31600 |
1.4401 |
X5CrNiMo17-12-2 | SUS316 |
06Cr17Ni12Mo2 |
316S31 |
| 316L | S31603 |
1.4404 |
X2CrNiMo17-12-2 |
SUS316L |
022Cr17Ni12Mo2 |
316S11 |
| 316Ti | S31635 |
1.4571 |
X6CrNiMoTi17-12-2 | SUS316Ti |
06Cr17Ni12Mo2Ti |
320S31 |
| 317 | S31700 |
1.4429 |
X5CrNiMo17-13-3 | SUS317 |
06Cr17Ni13Mo3 |
317S16 |
| 317L | S31703 |
1.4438 |
X2CrNiMo18-15-4 | SUS317L |
022Cr19Ni13Mo3 |
317L12 |
| 321 | S32100 |
1.4541 |
X6CrNiTi18-10 | SUS321 |
06Cr18Ni11Ti |
321S31 |
| 347 | S34700 |
1.4550 |
X6CrNiNb18-10 | SUS347 |
06Cr18Ni11Nb |
347S31 |
| 904L | N08904 |
1.4539 |
X1NiCrMoCu25-20-5 | - |
015Cr21Ni26Mo5Cu2 |
904S13 |
| AISI/ASTM | UNS | EN | DIN | JIS | GB (Lachin) | BS (UK) |
|---|---|---|---|---|---|---|
| 405 | S40500 | 1.4002 | X6CrAl13 | SUS405 |
06Cr13Al |
405S17 |
| 409 | S40900 | 1.4512 | X2CrTi12 | SUS409 |
06Cr11Ti |
- |
| 429 | S42900 | - | - | SUS429 |
10Cr15 |
- |
| 430 | S43000 | 1.4016 | X6Cr17 | SUS430 |
12Cr17 |
430S15 |
| 434 | S43400 |
1.4113 |
X6CrMo17-1 | SUS434 |
10Cr17Mo |
434S19 |
| 444 | S44400 |
1.4521 |
X2CrMoTi18-2 | SUS444 |
019Cr19Mo2NbTi |
- |
| 446 | S44600 | 1.4762 | X10CrAl24 | SUS446 |
16Cr25N |
- |
Martensitic Nerjaveèi klas ekivalan
| AISI/ASTM | UNS | EN | DIN | JIS | GB (Lachin) | BS (UK) |
|---|---|---|---|---|---|---|
| 410 | S41000 | 1.4006 | X12Cr13 | SUS410 |
12Cr13 |
410S21 |
| 416 | S41600 | 1.4005 | X12CrS13 | SUS416 |
Y12Cr13 |
416S21 |
| 420 (J1) | S42000 | 1.4021 | X20Cr13 | SUS420J1 |
20Cr13 |
420S29 |
| 420 (J2) | S42000 | 1.4028 | X30Cr13 | SUS420J2 |
30Cr13 |
420S37 |
| 431 | S43100 | 1.4057 | X17CrNi16-2 | SUS431 |
14Cr17Ni2 |
431S29 |
| 440A | S44002 | SUS440A |
68Cr17 |
- | ||
| 440B | S44003 | SUS440B |
75Cr17 |
- | ||
| 440C | S44004 | 1.4125 | X105CrMo17 | SUS440C | 95Cr18 | - |
| AISI/ASTM | UNS | EN | DIN | JIS | GB (Lachin) | BS (UK) |
|---|---|---|---|---|---|---|
| 2205 | S31803 / S32205 | 1.4462 | X2CrNiMoN22-5-3 | SUS329J3L | 022Cr23Ni5Mo3N | - |
| 2507 (Super Duplex) | S32750 | 1.4410 | X2CrNiMoN25-7-4 | - | 022Cr25Ni7Mo4N | - |
| AISI/ASTM | UNS | EN | DIN | JIS | GB (Lachin) | BS (UK) |
|---|---|---|---|---|---|---|
| 17-4PH | S17400 | 1.4542 | X5CrNiCuNb16-4 | SUS630 | 07Cr17Ni4Cu4Nb | - |
| 15-5PH | S15500 | 1.4545 | X5CrNiCuNb15-5 | SUS631J1 | 07Cr15Ni5Cu4Nb | - |
Ki ekivalan EN AISI 304 asye pur?
Ekivalan EN nan AISI 304 asye pur se EN 1.4301 (deziyasyon X5CrNi18-10). Nan sistèm DIN, sa a se konnen tou kòm Werkstoff Nr. 1.4301. ekivalan Japonè a se SUS304, ak ekivalan Chinwa GB a se 06Cr19Ni10 (ansyen 0Cr18Ni9). Tout deziyasyon sa yo refere a menm klas la ak apeprè 18% Kwòm ak 8% kontni nikèl.
Ki sa ki ekivalan Chinwa GB nan asye pur AISI 316?
Ekivalan Chinwa GB nan asye pur AISI 316 se 06Cr17Ni12Mo2 (ansyen deziyasyon: 0Cr17Ni12Mo2). Pou 316L, ekivalan GB a se 022Cr17Ni12Mo2 (ansyen deziyasyon: 00Cr17Ni12Mo2). Ekivalan EN yo se 1.4401 pou 316 ak 1.4404 pou 316L. Deziyasyon JIS Japonè yo se SUS316 ak SUS316L respektivman.
Èske SUS304 menm jan ak AISI 304?
Wi, SUS304 se deziyasyon JIS (Japanese Industrial Standards) pou menm klas ak AISI 304. Prefiks "SUS" la vle di "Steel Use Stainless" nan sistèm non JIS la. Tou de deziyasyon yo gen menm konpozisyon chimik (apeprè 18% chromium, 8% nikèl, mwens pase oswa egal a 0.08% kabòn) ak menm nimewo UNS S30400 la. Yo konplètman ka ranplase nan espesifikasyon materyèl.
Ki nimewo DIN pou asye pur 316L?
Nimewo DIN Werkstoff pou asye pur 316L se 1.4404 (deziyasyon X2CrNiMo17-12-2). Depi DIN estanda asye pur yo te lajman ranplase pa estanda EN (seri EN 10088), sa a se tou nimewo EN. Yon altènatif EN nimewo 1.4435 (X2CrNiMo18-14-3) tou pafwa referans pou 316L ak yon ti kras diferan konpozisyon ranje.
Èske klas asye pur ki soti nan diferan estanda egzakteman ki idantik?
Non. Klas ekivalan ki soti nan diferan estanda gen konpozisyon chimik ki sanble, men pa nesesèman idantik, ak pwopriyete mekanik. Ranje ki otorize pou eleman tankou kabòn, chromium, nikèl, ak molybdène ka diferan yon ti kras ant estanda ASTM, EN, JIS, ak GB. Pou egzanp, ranje a chromium pou "304" ta ka 18.0-20.0% nan ASTM men 17.5-19.5% nan EN. Pou aplikasyon kritik, toujou verifye limit konpozisyon egzak yo kont dokiman ofisyèl ofisyèl la epi konfime ak founisè ou a.
Kisa sifiks "L" vle di nan klas asye pur tankou 304L ak 316L?
"L" nan 304L ak 316L vle di "Low Carbon." Klas sa yo gen yon kontni maksimòm kabòn de 0.03% (konpare ak 0.08% nan estanda 304 ak 316). Kontni kabòn redwi minimize presipitasyon carbure (sansiblite) pandan soude, sa ki ka lakòz korozyon intergranular nan zòn ki afekte chalè a. Sa fè L-klas chwa pi pito pou konpozan soude ak konstriksyon gwo-kalib. Komèsyal la se yon ti kras pi ba tansyon ak fòs sede konpare ak klas estanda yo.