ASTM A213 TP316L Nerjaveèi asye chalè echanjeur tib

ASTM A213 TP316L Nerjaveèi asye chalè echanjeur tib

Estanda;ASTM A213 / ASME SA213
Klas;TP316L (UNS S31603)
Kalite Tib; Tib echanjeur chalè san pwoblèm
OD; 6.35-127 mm (1/4 "-5"), gwosè koutim ki disponib
WT; 0.4-12.7 mm
Longè; 3 m, 6 m, 12 m, U-Bend Tib oswa Customized
Fini andigman;Annealed & Pickled (AP), Bright Anileed (BA)
Fen; Plain Fen (PE), Bizote Fen (BE)
Kondisyon livrezon; Solisyon rkwit, marinated, trase frèt
Tretman Chalè; Solisyon rkwit Pi gran pase oswa egal a 1040 degre, Dlo Trempe
Fòm Tib; Tib Dwat, Tib U, Tib Bobin (Si ou vle)
Anbalaj; bouchon plastik, pakèt, ka an bwa, ekspòtasyon anbalaj maritim
Voye rechèch
Chat kounye a

ASTM A213 TP316L SS Tib Founisè, Manifakti, Ekspòtatè, Machann

GNEE gen plis pase 18 ane eksperyans nan fabrikasyon nan tib echanjeur chalè asye pur, li te apwovizyone tib asye pur a kliyan nan plis pase 80 peyi atravè lemond. Pwodwi nou yo sèvi divès sektè tankou pétrochimique, jenerasyon pouvwa, pwosesis manje, jeni maren, pharmaceutique, ak manifakti ekipman transfè chalè. Enstalasyon pwodiksyon nou yo opere an akò strik ak sistèm jesyon kalite ISO 9001. Pou chak pakèt ASTM A213 TP316L tib echanjeur chalè asye pur, nou bay EN 10204 3.1/3.2 Sètifika Tès Materyèl (MTC), asire trasabilite konplè soti nan matyè premyè rive nan pwodwi fini.

 

 EN 10204 3.1/3.2 Material Test Certificates (MTC)

Tib asye pur ASTM A213 TP316L nou bay yo se frèt -desine tib echanjeur chalè asye pur ki fèt espesyalman pou kondisyon sèvis segondè -tanperati ak segondè-. Ki gen 2%-3% molybdène (Mo) ak yon kontni kabòn ki ba (mwens pase oswa egal a 0.035%), klas sa a bay rezistans eksepsyonèl nan pike, korozyon fant, ak korozyon klori-pwovoke, pandan y ap asire ekselan soudabilite ak fyab alontèm-fonksyone nan anviwònman grav. Kontrèman ak tib soude, pwosesis fabrikasyon an san pwoblèm elimine kouti soude a, kidonk siyifikativman diminye risk ki genyen nan flit, konsantrasyon estrès, ak korozyon nan zòn nan soude.

 

Anplis de sa, tout tib 316L SS sibi yon pwosesis rkwir solisyon tanperati ki wo - nan tanperati ki depase 1040 degre ki te swiv pa refwadisman rapid. Sa a efektivman elimine estrès pwosesis entèn yo, estabilize estrikti austenitic la, epi kenbe dite tib anba a 95 HRB, sa ki fè yo pafètman apwopriye pou koube ki vin apre ak pwosesis agrandi tib.

 

Pou satisfè divès kondisyon konsepsyon echanjeur chalè, GNEE ofri tib ASTM A213 TP316L nan konfigirasyon miltip, ki gen ladan tib dwat, U{2}}tib koube, ak tib san pwoblèm bobin, ak sipò pèsonalizasyon konplè pou dyamèt eksteryè, epesè miray, longè, reyon koube, ak fini sifas. 316LU{4}tib soude soude nan entèn. echanjeur chalè-ak-tib, kidonk amelyore efikasite tèmik epi minimize pwen flit potansyèl yo. Pandan se tan, 316L san pwoblèm mawonnen tib kanpe kòm chwa ideyal pou echanjeur chalè kontra enfòmèl ant, kondansateur, sistèm instrumentation, ak ekipman pwosesis kontinyèl.

 

ASTM A213 TP316L Seamless Steel tubes
ASTM A213 TP316L Tib asye san pwoblèm
ASTM A213 TP316L Stainless Steel U-Tube
ASTM A213 TP316L Nerjaveèi U-tib
TP316L Stainless Steel Coiled Tube
TP316L Nerjaveèi asye mawonnen Tib

spesifikasyon

Atik Spesifikasyon
Estanda ASTM A213 / ASME SA213
Klas TP316L (UNS S31603)
Materyèl Austenitic Nerjaveèi
Dyamèt deyò (OD) 6.35-127 mm (1/4 "-5"), gwosè koutim ki disponib
Epesè miray (WT) 0.4-12.7 mm
Longè 3 m, 6 m, 12 m, U-Bend Tib oswa Customized
Sifas fini Rekwit & marinated (AP), Rekwit Bright (BA), Poli
Fini Fen Plain (PE), Fen Bizote (BE)
Kondisyon livrezon Solisyon rkwit, marinated, trase frèt
Tretman Chalè Solisyon rkwit Pi gran pase oswa egal a 1040 degre, dlo trempe
Fòm Tib Tib Dwat, Tib U, Tib Bobin (Si ou vle)
Anbalaj Bouchon plastik, pakèt, ka an bwa, ekspòtasyon anbalaj maritim
Enspeksyon 100% PMI, Tès Eddy aktyèl (ET), Tès idrostatik (HT), Tès à (UT), Tès Air anba dlo (Si ou vle)
Sètifikasyon EN 10204 3.1 / 3.2, ISO 9001, SGS, BV, TUV

 

Konpozisyon chimik:

Klas UNS C Mn P S Si Kr Ni Mo
TP316L S31603 0.035 max 2.00 max 0.045 max 0.03 max 1.00 max 16.0-18.0 10.0-14.0 2.00-3.00


Pwopriyete mekanik:

Klas Fòs Tensile, min, ksi (MPa)

Sede fòs,
min, ksi (MPa)

Elongasyon nan 2 pous.
oswa 50mm, min (%)

Dite

Tanperati solisyon,
min, degre F( degre)

Rockwell Brinell/Vickers
TP316L 70(485) 25(170) 35 90HRB 192HBW/200HV 1900(1040)

 

Spesifikasyon tolerans pou ASTM A213 TP316L Tib san pwoblèm

Gwosè Gwosè Gwosè   EstandaTolerans Tolerans Tolerans
Pwodwi yo OD Mi Longè ak/oswa bobin Klas OD Mi Longè
Chodyè asye Austenitic san pwoblèm,Sipèchofaj,
Tib Echanjeur Chalè ak Tib Kondansasyon Espesifikasyon: ASTM A213, ASME-SA213,ASTM-A688, ASME-SA688, ASTM A312, ASME SA 312
0.5 "(6 mm) a 12" (323.85 mm) gwosè metrik ki disponib 0.020 "(0.51 mm) a 1.312 " (33.325 mm) Longè o aza oswa koupe nan Kondisyon Kliyan 316/316L Under 1″ (25.4 mm) ±0.004″ (0.10 mm)1″ (25.4 mm) to 1-1/2″ (38.1 mm) ±0.006″ (0.15 mm)>1-1/2″ (38.1 mm) to 2″ (50.8 mm) ±0.008″ (0.20 mm)>2″ (50.8 mm) to 2-1/2″ (63.5 mm) ±0.010″ (0.25 mm)>2-1/2″ (63.5 mm) a 3″ (76.2 mm) ± 0.012″ (0.30 mm) 3″ (76.2 mm) a 4″ (101.6 mm) ± 0.015″ (0.38 mm) ±10% Owaza jiska +2″ (50.8 mm) Koupe +1/8″ (3 mm) -0″ Bobin a 80,000′ (24,384 m)

 

 

Klike pou telechaje fich done PDF ASTM A213 TP316L asye tiyo.

ASTM A213.PDF

ASTM A213.PDF

Aplikasyon pou TP316L san pwoblèm chalè echanjeur tib

Pwosesis chimik ak petwochimik: Yo itilize nan kondansateur, reyaktè enpòtan yo, ak kanalizasyon pwosesis pou jere asid korozif, solvang, ak likid presyon wo-.
Endistri lwil oliv ak gaz: Aplike nan platfòm lanmè ak enstalasyon pwosesis gaz natirèl.
Endistri jenerasyon pouvwa: Enstale nan kondansateur plant elektrik, sistèm rekiperasyon chalè nikleyè, ak sistèm vapè.

Applications Of ASTM A213 TP316L Stainless Steel Heat Exchanger Tubes:

 

Si ou gen kondisyon pwojè pou 316L tiyo asye pur, nou akeyi lòd ou yo. GNEE kenbe yon gwo envantè de pwodwi popilè pou ou pou w chwazi nan. Tanpri kontakte faktori nou jodi a; nou ofri pri konpetitif ak sèvis ekselan.

Kontakte kounye a

enspeksyon

Chak tib asye sibi 100% PMI (Idantifikasyon materyèl pozitif), analiz konpozisyon chimik, tès pwopriyete mekanik, tès kouran eddy oswa idrostatik, enspeksyon dimansyon, ak egzamen vizyèl anvan chajman. Chak pakèt lòd akonpaye pa yon Sètifika Tès Materyèl EN 10204 3.1 (MTC), epi yo ka bay sèvis enspeksyon twazyèm pati -SGS, BV, oswa TUV sou demann kliyan yo.

 TP316Tube
SS TP316 Tube
Dimensional Measurement
Mezi dimansyon
316 pipe PMI
316 tiyo PMI

anbalaj kalite siperyè

Anbalaj nan pake oswa kès plywood, vlope nan plastik, epi bay mezi pwoteksyon apwopriye pou asire konvnab pou transpò maritime, oswa chaje selon kondisyon espesifik.
Marking dwe konfòme yo ak dispozisyon ki nan Spesifikasyon A1016/A1016M epi endike si tiyo a cho -travay oswa frèt- travay; mak yo dwe gen ladan, men yo pa limite a: estanda, klas, gwosè, nimewo chalè, ak nimewo loto.

product-785-626
product-1706-1279

Feedback Kliyan

"Tub TP316L a gen ekselan konsistans dimansyon, ak pwosesis soude ak ekspansyon yo te lis, konplètman satisfè kondisyon nou yo pou tib echanjeur chalè. Rapò tès idrostatik konplè yo ak sètifika materyèl yo te ede nou pase enspeksyon twazyèm pati -." - Manadjè Teknik, Manifakti Echanjeur Chalè

ASTM A213 TP316L stainless steel heat exchanger tubes

FAQ

K. Ki diferans ki genyen ant ASTM A213 TP316L ak TP316?
A: TP316L gen yon maksimòm kontni kabòn de 0.030%, tandiske TP316 gen yon maksimòm de 0.08%. Kontni kabòn ki ba efektivman anpeche "presipitasyon carbure" pandan soude, kidonk evite korozyon entègranulè nan zòn nan soude. Malgre ke 316L ofri pi bon soudabilite, tanperati chanm li -fòs yon ti kras pi ba pase sa yo ki nan 316.

 

K. Èske yo ka itilize A213 TP316L pou tib Bend U-?
A: Wi. Nou souvan trete tib dwat A213 nan tib pliye U-. Fòme pliye a kreye estrès pwosesis nan zòn nan reyon (R-pliye). Tou depan de egzijans pwojè yo (tankou ASME B16.5), seksyon ki defòme nan U-koube a tipikman mande pou plis estrès-rekwit soulajman, ki te swiv pa tès 100% idrostatik oswa yon tès pasaj boul-.


K. Èske A213 TP316L ofri nenpòt avantaj pri sou A249 TP316L?
A: In fact, A213 (seamless) is more expensive than A249 (welded). A213 seamless tubes have no weld seams, offering greater safety in high-pressure environments (>5 MPa) ak elimine nesesite pou konsidere yon faktè efikasite jwenti soude; an konsekans, yo obligatwa nan endistri ki gen gwo-risk tankou lwil oliv ak gaz.

 

 

Baj popilè: ASTM A213 TP316L Nerjaveèi asye chalè echanjeur tib, Lachin ASTM A213 TP316L Nerjaveèi asye echanjeur chalè tib manifaktirè, Swèd, faktori