Estanda & Espesifikasyon
ASTM A249 \/ A269 \/ A213
En 10217-7 \/ en 10216-5
ISO 1127
ASME \/ PED \/ AD2 0 00 W0 Sètifikasyon ki disponib
ASTM A249 \/ A269 \/ A213 konpozisyon chimik
| Estanda | C (kabòn) | Si (Silisyòm) | MN (Manganèz) | P (fosfò) | S (souf) | Ni (nikèl) | Cr (CHROMIUM) | MO (MOLYBDENUM) | N (nitwojèn) |
|---|---|---|---|---|---|---|---|---|---|
| 304 (ASTM) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 0. 75 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 8.0 - 10.5 | 18.0 - 20.0 | - | Mwens pase oswa egal a 0. 01 |
| 304L (ASTM) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 0. 75 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 8.0 - 12.0 | 18.0 - 20.0 | - | Mwens pase oswa egal a 0. 01 |
| 316 (ASTM) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 0. 75 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 10.0 - 14.0 | 16.0 - 18.0 | 2.0 - 3.0 | Mwens pase oswa egal a 0. 01 |
| 316L (ASTM) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 0. 75 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 10.0 - 14.0 | 16.0 - 18.0 | 2.0 - 3.0 | Mwens pase oswa egal a 0. 01 |
| 430 (ASTM) | Mwens pase oswa egal a 0. 12 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 0. 040 | Mwens pase oswa egal a 0. 03 | - | 16.0 - 18.0 | - | - |
| SUS304 (JIS) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 8.0 - 10.5 | 18.0 - 20.0 | - | - |
| SUS304L (JIS) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 9.0 - 13.0 | 18.0 - 20.0 | - | - |
| Sus316 (jis) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 10.0 - 14.0 | 16.0 - 18.0 | 2.0 - 3.0 | - |
| Sus316l (jis) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 12.0 - 16.0 | 16.0 - 18.0 | 2.0 - 3.0 | - |
| SUS430 (JIS) | Mwens pase oswa egal a 0. 12 | Mwens pase oswa egal a 0. 75 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 0. 040 | Mwens pase oswa egal a 0. 03 | - | 16.0 - 18.0 | - | - |
| 06Cr19Ni10 (GB) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 8.0 - 11.0 | 18.0 - 20.0 | - | - |
| 022Cr19Ni10 (GB) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 8.0 - 12.0 | 18.0 - 20.0 | - | - |
| 06Cr17Ni12MO2 (GB) | Mwens pase oswa egal a 0. 08 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 10.0 - 14.0 | 16.0 - 18.0 | 2.0 - 3.0 | - |
| 022Cr17NI12MO2 (GB) | Mwens pase oswa egal a 0. 03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 03 | 10.0 - 14.0 | 16.0 - 18.0 | 2.0 - 3.0 | - |
| 10cr17 (GB) | Mwens pase oswa egal a 0. 12 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 0. 040 | Mwens pase oswa egal a 0. 03 | - | 16.0 - 18.0 | - | - |
| X5crni 18 - 10 (1.4301, en) | 0.07 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 015 | 8.0 - 10.5 | 17.5 - 19.5 | - | Mwens pase oswa egal a 0. 11 |
| X2crni 18 - 9 (1.4307, en) | 0.03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 015 | 8.0 - 10.0 | 17.5 - 19.5 | - | Mwens pase oswa egal a 0. 11 |
| X5crnimo 17 - 12 - 2 (1.4401, en) | 0.07 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 015 | 10.0 - 13.0 | 16.5 - 18.5 | 2.0 - 3.0 | Mwens pase oswa egal a 0. 11 |
| X2crnimo 17 - 12 - 2 (1.4404, en) | 0.03 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 015 | 10.0 - 13.0 | 16.5 - 18.5 | 2.0 - 3.0 | Mwens pase oswa egal a 0. 11 |
| X5crnimo 17 - 12 - 2 (1.4406, en) | 0.07 | Mwens pase oswa egal a 1. 00 | Mwens pase oswa egal a 2. 00 | Mwens pase oswa egal a 0. 045 | Mwens pase oswa egal a 0. 015 | 10.0 - 13.0 | 16.5 - 18.5 | 2.0 - 2.5 | Mwens pase oswa egal a 0. 11 |
Tib asye pur pou echanjeur chalè chofaj ak tretman sifas kondansateur
| Sijè | Sifas | Tib wonn - ASTM Creole |
|---|---|---|
| Mf | Kòm soude | |
| 180# | Buffed apre polisaj pa 180# | |
| 400# | Buffed apre polisaj pa 400# | |
| 600# | Buffed apre polisaj pa 600# | |
| De | Hairline fini apre polis pa 180#\/240# | |
| Tib kare ak rektangilè | Mf | Kòm soude |
| 180# | Buffed apre polisaj pa 180# | |
| 400# | Buffed apre polisaj pa 400# | |
| 600# | Buffed apre polisaj pa 600# | |
| De | Hairline fini apre polis pa 180#\/240# | |
| No.3 | Poli ak 100 - 120# senti abrazif | |
| No.4 | Poli ak 150 - 180# senti abrazif | |
| De | Te fè pa 150 - 320# abrazif senti fanm k'ap pile, modèl lineyè |
ASTM A249 \/ A269 \/ A213 EN 10217-7
| Epesè\/mm | 0.80 | 1.00 | 1.20 | 1.24 | 1.50 | 1.65 | 2.00 | 2.11 | 2.50 | 3.00 | 3.50 |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Kalib (pous) | 18GA | 16GA | 16GA | 14GA | 12GA | 11GA | |||||
| 9.50 (3/8) | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | |||
| 12.70 (1/2) | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | |||
| 15.90 (5/8) | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | |||
| 16.00 | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | |||
| 18.00 | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | ☆ | |||
| 19.10 (3/4) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 21.34 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 22.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 22.25 (7/8) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 25.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 25.40 (1) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 26.67 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 28.58 (1 1/8) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 31.80 (1 1/4) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 32.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 33.40 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 34.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 35.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | |||
| 38.10 (1 1/2) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 40.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 41.30 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 42.70 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 44.50 (1 3/4) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 48.26 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 48.60 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 50.80 (2) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 52.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 57.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 60.33 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 63.00 (2 1/2) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 70.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 76.20 (3) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 85.00 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 89.00 (3 1/2) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 101.60 (4) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 104.30 | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ | ||
| 114.30 (4 1/2) | ○ | ○ | ○ | ○ | ○ | ○ | ☆ | ☆ | ☆ |
Lejand:
☆ Reprezante pwosesis A249\/A269
○ reprezante pwosesis A269
△ Reprezante pwosesis A249\/A269 ki disponib
Se sèlman anndan chaplèt yo retire
Tib asye pur pou echanjeur chalè chofaj ak kondansateur nan stock

Aplikasyon pwodwi:Konstriksyon gwo presyon sou estasyon pouvwa chodyèr, tiyo surheatedsteam, tiyo dlo bouyi ak tiyo chofaj Locomotive.
Tès ak sètifikasyon
100% eddy aktyèl \/ tès idrostatik
PMI (verifikasyon materyèl)
ISO 9001: 2015 Kontwòl Kalite
PED \/ AD 2 0 00 W0 \/ ASME \/ CPR1090
3.1\/3.2 sètifika tès moulen bay yo
Kap chèchePremium tib asye purpou pwochen ouChodyè oswa chalè echanjeur pwojè? Kontakte nou pou yon quote, fich, oswa konsiltasyon teknik.
Voye rechèch