ASTM A268 Tp410 Tp430 Tp439 Tib Echanjeur Chalè Rekwit Bright

Mar 26, 2026

Kite yon mesaj

Poukisa se nan sèten pwojè echanjeur chalè ki enplike tanperati ki wo oswa anviwonman ki gen yon ti kras korozif-menm lè w ap itilize tib asye pur ki teknikman satisfè estanda endistri yo, pwoblèm tankou ekspansyon tib difisil, fann estrès soude, oswa efikasite echanj chalè enstab souvan parèt? Kòz la rasin souvan manti nan si kontwòl la nan tolerans dimansyon, inifòmite epesè miray la, ak fini sifas vrèman satisfè demand yo solid nan kondisyon fonksyònman sa yo.

 

Tib echanjeur chalè ASTM A268 TP410, TP430, ak TP439 Bright Annealed (BA) nou yo espesyalman fèt pou sistèm echanj chalè gwo -demann, ki ofri bon jan kalite fabrikasyon eksepsyonèl ak avantaj pèfòmans. Konsènan presizyon dimansyon, tout tib respekte estanda ASTM A268; tolerans dyamèt eksteryè a kontwole nan ± 0.3%, ak inifòmite epesè miray la se ekselan-ak devyasyon tipikman mwens pase oswa egal a 10%-kidonk asire sele serye pandan asanble fèy tib ak pwosesis ekspansyon, ak efektivman diminye risk pou yo mikwo{11}}devyasyon fant oswa fant inegal nan mi yo.

 
Pwodwi nou yo
 
ASTM A268 TP410 Heat Exchanger Tubes
ASTM A268 TP410 tib echanjeur chalè
ASTM A268 TP430 Tubes For Heat Exchanger
ASTM A268 TP430 tib pou echanjeur chalè
ASTM A268 TP439 Stainless Steel Tubes
ASTM A268 TP439 tib asye pur

 

An tèm de fini sifas, nou anplwaye yon pwosesis Bright Annealing (BA) pou asire yon wo degre de lis sou tou de sifas enteryè ak ekstèn nan tib yo, ak yon sifas brutality (Ra) tipikman mwens pase oswa egal a 0.8 μm. Sa a non sèlman diminye rezistans likid ak amelyore efikasite echanj chalè, men tou efektivman minimize tandans pou dekale ak korozyon, kidonk bay yon garanti solid pou fyab operasyon alontèm.

 

ASTM A268 TP410, TP430, TP439 Bright Annealed Chalè Echanjeur Espesifikasyon Tib

Dyamèt Deyò 6-203mm
Epesè miray la 0.5-25mm
Longè Jiska 25m
Estanda ASTM A268, ASME SA268
Klas TP410/TP405/TP420/TP430/TP430Ti/TP403/TP409/TP444/TP439/TP446, elatriye.
Kondisyon livrezon marinated, poli, klere rkwit
Teknik San pwoblèm/soude
Aplikasyon Echanjeur chalè, aparèy chofaj, kondansasyon, machinaj, machining kote yo pote, sèvis API...
Marking LOGO, Creole, Klas, Gwosè, Nimewo Chalè.
Pake Trikote sak, ka an bwa, oswa selon kondisyon kliyan an.
Kondisyon Kalite Sètifika Tès Mill (EN 10204/3.1); Twazyèm Pati Enspeksyon akseptab.

 

Konpozisyon chimik (poids %) pa ASTM A268

Eleman TP410 (UNS S41000) TP430 (UNS S43000) TP439 (UNS S43035)
Kabòn (C) 0.15% Max 0.12% Max 0.030% Max
Kwòm (Cr) 11.5 – 13.5% 16.0 – 18.0% 17.0 – 19.0%
Manganèz (Mn) 1.00% Max 1.00% Max 1.00% Max
Silisyòm (Si) 1.00% Max 1.00% Max 1.00% Max
Nikèl (Ni) 0.75% Max 0.75% Max 0.50% Max
Titàn (Ti) - - 1.10% Max*
Fosfò (P) 0.040% Max 0.040% Max 0.040% Max
Souf (S) 0.030% Max 0.030% Max 0.030% Max

 

Pwopriyete mekanik:

Pwopriyete TP410 TP430 TP439
Fòs rupture (MPa) Pi gran pase oswa egal a 415 (60 ksi) Pi gran pase oswa egal a 415 (60 ksi) Pi gran pase oswa egal a 415 (60 ksi)
Fòs Sede (MPa) Pi gran pase oswa egal a 205 (30 ksi) Pi gran pase oswa egal a 205 (30 ksi) Pi gran pase oswa egal a 205 (30 ksi)
elongasyon (nan 50mm) Pi gran pase oswa egal a 20% Pi gran pase oswa egal a 22% Pi gran pase oswa egal a 22%
Dite (Rockwell B) Mwens pase oswa egal a 90 HRB Mwens pase oswa egal a 89 HRB Mwens pase oswa egal a 89 HRB

 

Ki diferans prensipal ki genyen ant TP410, TP430, ak TP439?

TP410 se yon chalè-tretabl asye pur martensitic ki ofri rezistans korozyon modere, tandiske TP430 se yon 17% Cr-pote asye pur ferritik ki montre rezistans korozyon siperyè. TP439 se yon Titàn-estabilize feritik Nerjaveèi (ba-kabòn, segondè-chromium) ak rezistans korozyon menm plis eksepsyonèl, ki fèt espesyalman pou anpeche presipitasyon carbure.

 

Tès ki pa-destriktif

Tès Eddy Current: Bay 100% pwoteksyon pou detekte defo minit nan miray tib la.
Tès Idwostatik: Kenbe yon presyon estanda pou yon dire espesifik pou asire absans nenpòt ki koule.
Anplis de sa, nou ofri Air Under Water Testing, ki fèt espesyalman pou anviwònman ki enplike gaz trè pèmeyab.

430 Stainless Steel Pipe PMI
430 Nerjaveèi asye tiyo PMI
Hydrostatic Testing
Tès idrostatik

Anbalaj ak make:

Pwodwi yo dwe pake nan pake oswa kès plywood, vlope nan plastik, epi yo dwe bay mezi pwoteksyon apwopriye pou asire transpò maritime, oswa pake an akò ak kondisyon espesifik.
Mak yo dwe endike si tiyo a cho-travay oswa frèt-, epi yo dwe gen ladan-men pa limite a-enfòmasyon sa yo: estanda, klas, dimansyon, nimewo chalè, ak nimewo pakèt.

Stainless Tubes Packing by Wooden Box
Tib Nerjaveèi anbalaj pa bwat an bwa
Standard export wooden crate packaging
Estanda ekspòtasyon an bwa kès anbalaj

Voye rechèch