ASTM A240 TP304 / 304L / 304H Plak asye pur nan stock
Oct 21, 2025
Kite yon mesaj
GNEE bay gwo -bon jan kalite ASTM A240 TP304, 304L, ak 304H plak asye pur pou yon pakèt aplikasyon nan sektè chimik, manje, pétrochimique, ak endistriyèl. Plak sa yo fabrike nan estanda entènasyonal yo epi yo ofri ekselan rezistans korozyon, fòs mekanik, ak rezistans.
GNEE ofri tou de -stock envantè ak gwosè koutim pou satisfè bezwen pwojè ou yo, asire livrezon rapid. Nou ofri sa ki annapre yo: plak AISI 304, UNS S30400 plak, 304/304L/304H asye pur fèy / teren / bobin, 304 Nerjaveèi asye frèt -plak -040}woule, asye pur, woule cho{10}. 304 Nerjaveèi asye plak karo, 304 Nerjaveèi asye plak detache, 304 Nerjaveèi asye plak Relief, 304 Nerjaveèi asye poli plak, 304 Nerjaveèi asye bwose plak, 304 Nerjaveèi asye plak glas, 304 Nerjaveèi asye plak san pwoblèm, 304 Nerjaveèi asye soude plak, ak plis ankò.
Ki diferans ki genyen ant TP304, TP304L, ak TP304H?
TP304 - Estanda austenitic Nerjaveèi, ideyal pou aplikasyon jeneral korozyon -rezistan.
TP304L - Variant ki ba kabòn, ki fèt pou aplikasyon pou soude ak redwi risk pou korozyon entègranulèr.
TP304H - Variant segondè kabòn, apwopriye pou sèvis tanperati ki wo, kenbe fòs nan tanperati ki wo.
Plak yo disponib nan epesè soti nan 1 mm a 300 mm, ak divès kalite fini sifas ki gen ladan 2B, BA, No.4 fwote, ak glas poli.

ASTM A240 TP304 / 304L / 304H Spesifikasyon plak asye pur
| Estanda |
ASTM A240/A240M |
|---|---|
| Klas |
1.4301/1.4307/1.4948, SUS 304/304L/304H |
| Longè |
2000 mm - 6000 mm (78.74 "- 236.22"), Customized |
| Epesè |
0.3 mm - 100 mm (0.012 "- 3.937"), Customized |
| Lajè |
1000 mm - 2000 mm (39.37 "- 78.74"), Customized |
| Sifas fini |
2B, 2D, 8K, BA, karo, Customized, Relief, grave, liy cheve, glas, No.1, No.4, No.8, sab eksplozyon |
| Teknik |
Recuit, woule frèt, koupe, woule cho |
| Fòm |
Plak karo (plak Diamond), plak rekouvèr, bobin, Customized, plak plat, plak pèse, fèy, teren, plak teksti |
Konpozisyon chimik
| Klas | Kwòm (Cr) | Nikèl (Ni) | Kabòn (C) | Manganèz (Mn) | Silisyòm (Si) | Fosfò (P) | Souf (S) |
|---|---|---|---|---|---|---|---|
| 304 | 18.0-20.0% | 8.0-10.5% | Mwens pase oswa egal a 0.08% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
| 304L | 18.0-20.0% | 8.0-12.0% | Mwens pase oswa egal a 0.03% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
| 304H | 18.0-20.0% | 8.0-12.0% | Mwens pase oswa egal a 0.04% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
Pwopriyete mekanik
| Pwopriyete | 304 | 304L | 304H |
|---|---|---|---|
| Fòs rupture | 515 - 750 MPa (75 - 108.8 ksi) | 485 - 700 MPa (70 - 101.5 ksi) | 515 - 750 MPa (75 - 108.8 ksi) |
| Sede fòs | 205 MPa (30 ksi) | 170 MPa (25 ksi) | 275 MPa (40 ksi) |
| Dite Brinell (HBW) | 123 – 201 | 123 – 201 | 123 – 201 |
| Rockwell Hardness (HRB) | 70 – 90 | 70 – 90 | 70 – 90 |
| Vickers dite (HV) | 129 – 210 | 129 – 210 | 129 – 210 |
| Allongement nan Break | 40% | 40% | 40% |
| Modil Young la | 193 - 200 GPa (28 - 29 msi) | 193 - 200 GPa (28 - 29 msi) | 193 - 200 GPa (28 - 29 msi) |
Analiz mache ak pri
304 plak asye pur retetrè mandenan sektè endistriyèl ak komèsyal akòz yofyab, rezistans korozyon, ak adaptabilite.
Ranje pri apwoksimatif (USD/kg):
1-10 mm epesè: $3.5 - $4.5 pou chak kg
10-50 mm epesè: $4.0 - $5.0 pou chak kg
50-300 mm epesè: $4.5 - $6.0 pou chak kg
Pri yo varye selon kondisyon mache yo, depans nikèl ak chromium, ak kantite lòd. Lòd en oswa koutim ka resevwa rabè. Imèl:sales@gneestainless.com
GNEE faktori fòs
Etablisman pwodiksyon 50,000+ m² ak ekipman avanse woule, tretman chalè, koupe, ak polisaj.
ISO 9001, SGS, ak BV sètifye plak asye pur.
100% tès bon jan kalite: PMI, ultrasons, mekanik, ak tès korozyon.
Gwo disponiblite stock pou livrezon imedya, epesè miltip ak fini sifas yo.
Custom fabrikasyon: koupe, koupe, tretman chalè, sèvis polisaj ki disponib.
Anbalaj ak livrezon
Chak plak vlope ak papye anti-rouye, fim PVC, ak palèt an bwa pou transpò an sekirite.
Gad Edge pwoteje kwen pandan anbake.
Tan livrezon: 7-15 jou travay pou plak ki estoke.
Tèm livrezon: FOB, CIF, EXW, DDP.
Tèm peman: T/T (30% davans, 70% anvan chajman), L/C, Western Union.

Voye rechèch