Ki sa ki 2205 alyaj asye pur cho -woule plak?
2205 alyaj Nerjaveèi asye plak woule cho -(UNS S32205, EN 1.4462, ASTM A240/A240M) se yon feritik-austenitic duplex plak asye pur ak yon jisteman balanse 50-50 mikwostrikti, ki montre severite enpak nan -4000000. valè 32-36 (ekselan rezistans korozyon pitting nan anviwònman maren/klori). Li fabrike nan woule cho ki te swiv pa rkwir solisyon nan 1020-1100 degre ak trempe dlo. Li se lajman ki itilize nan platfòm lwil oliv ak gaz lanmè, plant desalination, ekipman chimik, ak veso presyon.
GNEE se yon founisè serye ak manifakti nan 2205 tiyo asye pur, plak, fèy, ak ba ki soti nan Lachin. Nou bay sèvis pwosesis Customized pou divès kalite pwodwi asye pur 2205, ki gen ladan koupe, soude, polisaj, tretman chalè, ak plis ankò.
Pwodwi nou yo gen ladan yo: 2205 cho -woule plak asye pur, 2205 frèt- plak woule, 1.4462 tiyo san pwoblèm, 2205 tiyo soude, 318S13 plak poli, 2205 plak bwose, S32205 plak wonn, 20 ba kare, ba 252525 2205 ba kre.
Nou bay 2205 duplex Nerjaveèi asye cho -woule plak ak epesè ki sòti nan 4.5-100 mm (mwayen plak: 4.5-20 mm, plak epè: 20-100 mm), lajè soti nan 1500-2500 mm, ak longè soti nan 6000-1200 mm, ak sifas ki soti nan 6000-1200. Mwens pase oswa egal a 12.5 μm).
Pwodwi nou yo
Si ou vle konnen plis detay ak pri nan pwodwi yo, tanpri kontakte nou nan tan!sales@gneestainless.com



Espesifikasyon pou 2205 alyaj asye pur cho -woule plak
| Estanda |
ASTM A240, ASTM A480 |
|---|---|
| Klas |
1.4462, 318S13, S32205, X2CrNiMoN22-5-3 |
| Longè |
2 m-12 m (6.6-40 pye), Customized |
| Epesè |
Customized, Plak: 5 mm-150 mm (0.2-6 nan), Fèy: 0.5 mm-5 mm (0.02-0.2 nan) |
| Tout Lajè |
Customized, Plak: 1000 mm-3000 mm (39.37-118.11 nan), Fèy: 1000 mm-2000 mm (39.37-78.74 nan) |
| Dyamèt |
Bar: 6 mm-600 mm (0.24-24 nan), Customized |
| Fòm |
Customized, elatriye, plat, oval, tiyo & Bar: wonn, rektangilè, kare |
| Sifas fini |
BA, Nwa, Customized, Non . 2D, No.1, No.4, marinated, Poli |
Konpozisyon chimik
| Kabòn (C) |
|
Fosfò (P) | Souf (S) | Silisyòm (Si) | Kwòm (Cr) |
|
Molybdène (Mo) | Azòt (N) | ||
|---|---|---|---|---|---|---|---|---|---|---|
| Mwens pase oswa egal a 0.03 | Mwens pase oswa egal a 2.00 | Mwens pase oswa egal a 0.03 | Mwens pase oswa egal a 0.02 | Mwens pase oswa egal a 1.00 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.14-0.20 |
Pwopriyete mekanik
| Pwopriyete mekanik | Valè (metrik) | Valè (Enperyal) |
|---|---|---|
| Fòs rupture | 515-720 MPa | 74,700-104,400 psi |
| Sede fòs | 205 MPa | 29,700 psi |
| Dite Brinell (HB) | 150-220 HB | 150-220 HB |
| Rockwell Hardness (HRC) | 20-30 HRC | 20-30 HRC |
| Vickers dite (HV) | 160-220 HV | 160-220 HV |
| Elongasyon | 40-60% | 40-60% |
| Modil elastik | 193-200 GPa | 28,000-29,000 ksi |
| Regleman | Spesifikasyon |
|---|---|
| Kantite minimòm lòd: | 5 tòn |
| Pri: | Pou negosye |
| Detay anbalaj: |
Jan yo mande |
| Tan livrezon: | Nan 7-10 jou travay |
| Kondisyon Peman: | T/T, L/C, Kat kredi |
| Kapasite Pwovizyon pou: | 100000 Tòn pa mwa |
| Sètifikasyon: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
2205 Duplex Nerjaveèi asye plak pri
| 2205 Duplex Nerjaveèi asye plak pri pou chak kg | pou chak inite (usd) |
|---|---|
| 2205 duplex 2000mm x 1000mm x 3mm plak thk | 4.59 |
| 300 mm dyamèt ak 4mm epesè duplex 2205 plak | 30.45 |
| 2mm x 102mm x 316mm duplex 2205 plak | 3.29 |
| duplex 2 mm x 51mm x 250mm plak | 3.21 |
| 2mm x 102mm x 385mm duplex 2205 plak | 3.66 |
| duplex 2205 2mm x 102mm x 351mm plak | 3.51 |
2205 plak asye pur yo trete lè l sèvi avèk ekipman pwodiksyon avanse, asire presizyon ak konsistans nan chak plak. Faktori a itilize zouti ki wo -efikasite tankou machin koupe lazè, machin pwensonaj CNC, ak ekipman polisaj, ki kapab trete plak asye pur nan espesifikasyon divès kalite ak epesè ki sòti nan 0.3mm a 8mm, epi asire ke pwodwi yo satisfè estanda entènasyonal tankou ASTM A240. Anvan chajman, chak pakèt sibi bon jan kalite tès solid, ki gen ladan chèk sou fini sifas, tolerans epesè, ak presizyon dimansyon, asire ke pwodwi yo satisfè kondisyon kliyan yo.

An tèm de anbalaj ak transpò, tout plak asye pur yo trete ak mezi prèv imidite -e yo pake san danje lè l sèvi avèk kès an bwa, palèt, oswa vlope jarèt. Kontenè estanda oswa machin transpò dedye yo itilize pou transpò, asire entegrite ak sekirite machandiz yo pandan transpò. Nou ofri anbake atravè lemond, ak yon tan livrezon tipik nan 7-15 jou soti nan pwodiksyon an livrezon, asire livrezon alè nan kliyan nou yo.

Voye rechèch