Zouti Atelye: 440C vs 410 kle & lam
Jun 30, 2025
Kite yon mesaj



Poukisa bon kouto 440C?
Segondè kabòn (1.2%) kenbe précision. Dite rive nan 58 HRC - dire 5x pi long pase asye bon mache. Siye apre koupe manje asid.
Èske 410 Nerjaveèi ka fè kle dirab?
Wi, men mwens difisil pase asye chrome-vanadyòm. Pa pral rouye lè lwil. Pi bon pou Rahman itilize zouti.
Kenbe lam wè?
Pitch pwòp ak cleaner fou. Sere sèk pou anpeche korozyon. Egwize lè koupe santi "draggy."
Poukisa kèk pens rouye?
Gen anpil chans 420J2 Steel - Minimal CHROMIUM. Upgrade a 410 oswa kenbe alalejè wile.
Brikoleur file konsèy?
Sèvi ak wòch dyaman pou 440C. 20 degre ang pou kouto. Pa chofe - pant nan dlo yo refwadi.