TP304L vs TP316L: Konpozisyon & diferans kle
Aug 07, 2025
Kite yon mesaj
Ki sa kiTP304L?
ASTM A312 TP304L se yon klas austenitic ki ba -kabòn ki fèt ak yon konpozisyon siperyè nikèl ak chromium, ki bay rezistans amelyore kont medya korozif ak oksidatif. Tiyo sa yo gen plis fòs epi yo ka travay nan konfigirasyon tanperati ki wo
Ki sa ki materyèl TP316L?
A312 TP316L se klas austenitic ki ba -kabòn ki pwodui ak nikèl, chromium ak molybdène (2.0-3.0%). Anplis molybdène a bay siperyè kowozyon ak oksidasyon rezistans, patikilyèman kont klori, pitting ak kreve korozyon - fè 316L estanda pou sèvis maren, bò lanmè ak chimik.
Tou de TP304L (UNS S30403) ak TP316L (UNS S31603) se klas tiyo asye pur austenitic ba-kabòn ki kouvri anba ASTM A312. Lèt "L" la vle di kabòn ki ba (max 0.03%), minimize presipitasyon carbure ak korozyon entègranulè apre soude.
Materyèl ekivalannan TP304L ak TP316L
|
ASTM A312 Klas
|
EN (Ewòp)
|
DIN (Almay)
|
JIS (Japon)
|
GB (Lachin)
|
|---|---|---|---|---|
|
TP304L
|
EN 1.4307 / X2CrNi18-9
|
1.4307
|
SUS304L
|
022Cr19Ni10
|
|
TP316L
|
EN 1.4404 / X2CrNiMo17-12-2
|
1.4404
|
SUS316L
|
022Cr17Ni12Mo2
|
Konpozisyon chimik TP304L ak TP316L (% wt, ASTM A312)
| Eleman | TP304L (S30403) | TP316L (S31603) |
|---|---|---|
| Kabòn (C) | Mwens pase oswa egal a 0.03 | Mwens pase oswa egal a 0.03 |
| Kwòm (Cr) | 18.0‑20.0 | 16.0‑18.0 |
| Nikèl (Ni) | 8.0‑13.0 | 10.0‑14.0 |
| Molybdène (Mo) | ‑ | 2.0‑3.0 |
| Manganèz (Mn) | Mwens pase oswa egal a 2.00 | Mwens pase oswa egal a 2.00 |
| Silisyòm (Si) | Mwens pase oswa egal a 1.00 | Mwens pase oswa egal a 1.00 |
| P / S | Mwens pase oswa egal a 0.045 / Mwens pase oswa egal a 0.030 | Mwens pase oswa egal a 0.045 / Mwens pase oswa egal a 0.030 |
| Fè | Balans | Balans |
Kle diferans alyaj: TP316L gen 2.0-3.0% molybdène, ki TP304L pa genyen. Molybdène anpil amelyore rezistans nan twou klori-pwovoke ak korozyon fant. Valè PREN: TP304L ≈18‑20; TP316L ≈24.
Pwopriyete mekanik TP304L ak TP316L (Solisyon-Annealed, Tanperati chanm, ASTM A312 Minimòm)
| Pwopriyete | TP304L | TP316L |
|---|---|---|
| Fòs rupture (MPa) | Pi gran pase oswa egal a 485 | Pi gran pase oswa egal a 485 |
| Fòs Sede (0.2%, MPa) | Pi gran pase oswa egal a 170 | Pi gran pase oswa egal a 170 |
| elongasyon (%) | Pi gran pase oswa egal a 35 | Pi gran pase oswa egal a 35 |
| Dite (HRB) | Mwens pase oswa egal a 90 | Mwens pase oswa egal a 90 |
Remak: Pwopriyete mekanik tanperati chanm yo fèmen pou tou de klas yo. Diferans nan pi gwo manti nan pèfòmans korozyon olye ke fòs.
Pwopriyete fizik TP304L ak TP316L
| Pwopriyete | TP304L | TP316L |
|---|---|---|
| Dansite (g/cm³) | 8.00 | 7.99 |
| Pwen fizyon (degre) | 1400–1450 | 1370–1400 |
| Kondiktivite tèmik (W/m·K) | 16.2 (nan 100 degre) | 16.3 (nan 100 degre) |
| Chalè espesifik (J/kg·K) | 500 | 500 |
| Rezistans elektrik (μΩ·cm) | 72 | 74 |
Diferans pèfòmans kle nan TP304L ak TP316L