SUS317 Nerjaveèi: Amelyore Molybdène pou korozyon grav

Jan 22, 2026

Kite yon mesaj

304 Stainless Steel Round Bar and tubeBright Annealed Polished ASTM A269 316L Stainless steel Seamless TubingsSUS304H Stainless Steel: High-Carbon Grade for Elevated Temperatures

Konpozisyon chimik

Konpozisyon chimik klas 317 asye pur endike nan tablo ki anba la a.

Eleman Kontni (%)
Iron, Fe 61
Kwòm, Kr 19
Nikèl, Ni 13
Molybdène, Mo 3.50
Manganèz, Mn 2
Silisyòm, Si 1
Kabòn, C 0.080
Fosfò, P 0.045
Souf, S 0.030

 

 

Pwopriyete Fizik

Tablo ki anba la a montre pwopriyete fizik klas 317 asye pur.

Pwopriyete Metrik Imperial
Dansite 8 g/cm3 0.289 lb/pous³
Pwen k ap fonn 1370 degre 2550 degre F

 

 