630 (17-4 PH) vs 15-5 PH (XM-12) Precipitation-Hardening Stainless Steels: Versatile vs High-Toughness Strength410 vs 430 Martensitic vs Ferritic Stainless Steels: Weldable Strength vs Decorative Cost-Effectiveness309S vs 310S Austenitic Stainless Steels: High-Temp Oxidation vs Extreme Heat Resistance

Konpozisyon chimik nan asye pur 304

Tablo 1.Konpozisyon chimik pou 304 alyaj asye pur

%

304

304L

304H

C

0.0 - 0.07

0.0 - 0.03

0.04 - 0.08

Mn

0.0 - 2.0

0.0 - 2.00

0.0 - 2.0

Si

0.0 - 1.00

0.0 - 1.00

0.0 - 1.0

P

0.0 - 0.05

0.0 - 0.05

0.0 - 0.04

S

0.0 - 0.03

0.0 - 0.02

0.0 - 0.02

Kr

17.50 - 19.50

17.50 - 19.50

17.00 - 19.00

Ni

8.00 - 10.50

8.00 - 10.50

8.00 - 11.00

Fe

Balans

Balans

Balans

N

0.0-0.11

0.0-0.11

0.0 - 0.10

 

Nerjaveèi asye 304 gen ekselan rezistans korozyon nan yon gran varyete anviwònman ak lè an kontak ak diferan medya korozivite. Pitting ak kreve korozyon ka rive nan anviwònman ki gen klori. Krak korozyon estrès ka rive nan tanperati ki depase 60 degre.

 