What is 1.4833 Stainless Steel?Grade comparisons of 410 stainless steelsStainless Steel - Grade 347 - AISI 347 Fe/Cr18/Ni10/Nb (UNS S34700)

🧪 Konpozisyon Chimik

Eleman Konpozisyon (%)
Kabòn (C) 0.04 - 0.10
Manganèz (Mn) Mwens pase oswa egal a 2.00
Silisyòm (Si) Mwens pase oswa egal a 0.75
Fosfò (P) Mwens pase oswa egal a 0.045
Souf (S) Mwens pase oswa egal a 0.030
Kwòm (Cr) 16.0 - 18.0
Nikèl (Ni) 10.0 - 14.0
Molybdène (Mo) 2.0 - 3.0
Azòt (N) Mwens pase oswa egal a 0.10
Fè (Fe) Balans

⚙️ Pwopriyete mekanik

Pwopriyete Valè
Fòs rupture (tanperati chanm) Pi gran pase oswa egal a 515 MPa
Fòs Sede (0.2% Offset) Pi gran pase oswa egal a 205 MPa
Elongasyon (50mm kalib) Pi gran pase oswa egal a 40%
Rediksyon nan zòn Pi gran pase oswa egal a 50%
Dite (Brinell) Mwens pase oswa egal a 217 HB
Dite (Rockwell B) Mwens pase oswa egal a 95 HRB
Enèji enpak (Charpy V-dan, 20 degre) Pi gran pase oswa egal a 120 J
Limit Fatig (107sik) 240 MPa
Modil Young la 200 GPa
Chea modil 81 GPa

🔬 Pwopriyete Fizik

Pwopriyete Valè
Dansite (20 degre) 8.0 g/cm³
Pwen k ap fonn 1400-1450 degre
Kondiktivite tèmik (20 degre) 16.2 W/m·K
Kondiktivite tèmik (100 degre) 17.5 W/m·K
Ekspansyon tèmik (20-100 degre) 16.0×10-6/K
Ekspansyon tèmik (20-300 degre) 17.0×10-6/K
Chalè espesifik (20 degre) 500 J/kg·K
Rezistans elektrik (20 degre) 0.74 µΩ·m
Pèmeyabilite mayetik 1.02 µr (max)
Tanperati Curie Ki pa-mayetik

📏 Espesifikasyon pwodwi yo

Spesifikasyon Opsyon ki disponib
Fòm pwodwi Ba wonn, ba plat, plak, dra, tib, tiyo, forgings, depoze
Round Bar Dyamèt 6mm - 300mm
Flat Bar Dimansyon 10×3mm - 150×50mm
Epesè plak 3mm - 100mm
Epesè fèy 0.5mm - 3mm
Dyamèt Eksteryè Tib 6mm - 219mm
Konfòmite estanda ASTM A240, A276, A312, A479, EN 10088, JIS G4303, GB/T 1220
Fini andigman Woule cho, trase frèt, rkwit klere, marinated, poli (2B, BA, No.4)
Dimansyon tolerans ± 0.1mm a ± 0.5mm (depann sou fòm pwodwi)
Opsyon Longè Longè estanda: 3m, 6m, 12m; Longè koutim ki disponib