ASME SA213 TP304 Stainless Steel Seamless Heat Exchanger TubeASME SA268 TP410 Bright Annealed Seamless TubeASME SA268 TP430 Stainless Steel Heat Exchanger Tube

Konpozisyon chimik

Eleman Konpozisyon (%)
Kabòn (C) Mwens pase oswa egal a 0.030
Kwòm (Cr) 21.0 - 23.0
Nikèl (Ni) 4.5 - 6.5
Molybdène (Mo) 2.5 - 3.5
Azòt (N) 0.08 - 0.20
Manganèz (Mn) Mwens pase oswa egal a 2.00
Silisyòm (Si) Mwens pase oswa egal a 1.00
Fosfò (P) Mwens pase oswa egal a 0.035
Souf (S) Mwens pase oswa egal a 0.020

⚙️ Pwopriyete mekanik

Pwopriyete Valè
Fòs Sede (MPa) Pi gran pase oswa egal a 450
Fòs rupture (MPa) 620 - 880
elongasyon (%) Pi gran pase oswa egal a 25
Dite (HRC) 22 - 28
Tanperati Kritik Pitting (degre) Pi gran pase oswa egal a 35
Valè PREN Pi gran pase oswa egal a 35
Enèji enpak nan -40 degre (J) Pi gran pase oswa egal a 60