Biopharmaceutique byoreactors: 316L vs . 904 L Cleanability

Jun 23, 2025

Kite yon mesaj

316L vs. 904L stainless steel316L vs. 904L stainless steel316L vs. 904L stainless steel

 

Poukisa 316L-EP domine kilti selil mamifè yo?
Electropolishing a RA 0 . 25μm diminye adsorption pwoteyin pa 80%. pasivated pou chak ASTM A967 elimine fè gratis . valide pou 300+ SIP CYCLES nan 130 degre {{{}}}}}}.

 

Lè 904L obligatwa pou medya agresif?
Pou solisyon tanpon asid (ph<4) or high-chloride feeds. Molybdenum (4.5%) prevents pitting during CIP with 2M NaOH/1M HCl. Copper addition (1.5%) improves sulfuric acid resistance for cleaning validation.

 

Sifas validasyon brutality?
RA mwens pase oswa egal a 0 . 4μm pou aplikasyon pou kilti selil yo. Rmax<2μm per ASME BPE-2019. No peaks >0 . 5μm sou 10mm longè eskanè . blan limyè interferometri pou kat sifas 3D.

 

Pwotokòl tès pwòp?
Tès adezyon serom bovin<5 μg/cm². Endotoxin recovery <0.25 EU/mL after sterilization. TOC rinse water analysis <500 ppb. Biofilm challenge with Pseudomonas aeruginosa.

 

Soudure pi bon pratik?
Orbital gtaw ak ER316LSI filler . entèn argon wete bagay o₂<50ppm. No crevices allowed (weld reinforcement <10% wall thickness). Post-weld electropolishing of all product contact zones.