What is SAE 904L stainless steel sheet?410 Stainless Steel Plate & Coil: Martensitic Wear-Resistant Industrial Plate/Coil347 Stainless Steel Pipe & Tube: Niobium-Tantalum Stabilized High-Temp Corrosion Resistant Piping321 Stainless Steel Pipe & Tube: Titanium-Stabilized Post-Weld Corrosion Resistant Piping

Konpozisyon

Tablo ki anba a bay seri konpozisyon klas 904L asye pur:

Tablo 1. Ranje konpozisyon nan klas 904L asye pur

Klas C Mn Si P S Kr Mo Ni Cu
904L

min.

max.

-

0.02

-

2

-

1

-

0.045

-

0.035

19

23

4

5

23

28

1

2

Pwopriyete mekanik

Pwopriyete mekanik tipik nan asye pur klas 904L yo bay nan tablo ki anba a:

Tablo 2. Pwopriyete mekanik nan klas 904L asye pur

Klas Fòs rupture (MPa) min Sede fòs 0.2% Prèv (MPa) min Elongasyon (% nan 50mm) min Dite
Rockwell B (HR B) Brinell (HB)
904L 490 220 36 70-90 tipik 150

Pwopriyete Fizik

Pwopriyete fizik klas 904L asye pur yo tabli anba a:

Tablo 3. Pwopriyete fizik tipik nan asye pur klas 904L

Klas Dansite
(kg/m3)
Modil elastik
(GPa)
Mwayèn Ko-efè ekspansyon tèmik (µm/m/ degre) Kondiktivite tèmik
(W/m.K)
Espesifik Chalè 0-100 degre
(J/kg.K)
Rezistivite elektrik
(nΩ.m)
0-100 degre 0-315 degre 0-538 degre Nan 20 degre Nan 500 degre
904L 7900 190 15 - - 11.5 - 500 952

Konparezon Spesifikasyon Klas

Tablo sa a montre konparezon klas apwoksimatif asye pur 904L:

Tablo 4. Espesifikasyon klas nan asye pur klas 904L

Klas UNS No Old Britanik Euronorm Swedish SS Japonè JIS
BS En Non Non
904L N08904 904S13 - 1.4539 X1NiCrMoCuN25-20-5 2562 -