ASTM A213 TP347 Nerjaveèi asye tiyo san pwoblèm

Jan 27, 2026

Kite yon mesaj

ki sa ki ASTM A213 TP347?

ASTM A213 TP347 se yon niobyòm -tantal estabilize austenitic Nerjaveèi asye tiyo san pwoblèm, ak pi bon segondè -estabilite tanperati pase Titàn-estabilize klas. Li se lajman ki itilize nan nikleyè, pouvwa ak gwo -tanperati pwosesis echanjeur chalè tib.

Klas ekivalan (orizontal)

UNS: S34700|JIS: SUS347|GB: 06Cr18Ni11Nb|EN: X6CrNiNb18-10|W.Nr.: 1.4550

Konpozisyon chimik (pwès%, orizontal)

C: Mwens pase oswa egal a 0.08|Si: Mwens pase oswa egal a 1.00|Mn: Mwens pase oswa egal a 2.00|P: Mwens pase oswa egal a 0.045|S: Mwens pase oswa egal a 0.030|Cr: 17.00-19.00|Ni: 9.00-13.00|Nb+Ta: Pi gran pase oswa egal a 10×C|Fe: Balans

Pwopriyete kle (20 degre, rkwit, orizontal)

Dansite: 7.93g/cm³|Pwen k ap fonn: 1400-1450 degre|Fòs Tensile: Pi gwo pase oswa egal a 515N/mm²|Fòs Sede: Pi gwo pase oswa egal a 205N/mm²|Elongasyon: Pi gran pase oswa egal a 40%|Dite: Mwens pase oswa egal a 201HB

Karakteristik debaz yo

• Niobyòm-estabilizasyon Tantal bay siperyè apre-soude rezistans korozyon entègranulè ak estabilite segondè-tanperati • Ekselan segondè-tanperati rezistans ranpe, apwopriye pou sèvis alontèm -tèm jiska 900 degre • Bon soudabilite ak estabilite estriktirèl, pa gen okenn evidan, pèfòmans nikleyè segondè {6}degradasyon nikleyè; founo ak aplikasyon pou tiyo pwosesis kritik

TP347 vs TP321 (Orizontal)

Estabilize: 347 (Nb+Ta)|321 (Ti)|Segondè -Estabilite Tanperati: 347 (Siperyè)|321 (Bon)|Ranpe Rezistans: 347 (Pi bon)|321 (Jeneral)|Aplikasyon: 347 (Nikleyè/Segondè-Fen)|321 (Jeneral High-Temp)

UNS No Klas C Si Mn P S Kr Mo Ni N Lòt
S34700 347 0.08 0.75 2.00 0.045 0.030 17.00/19.00 – 9.00/13.00 – Cb:10xC1.00

 

Founisè asye pur

Si ou gen kondisyon pwojè pou asye pur, nou akeyi lòd ou a. GNEE gen yon gwo envantè de pwodwi popilè pou ou pou w chwazi. Li ka trete nan divès fòm pwodwi pratik, ki gen ladan plak, bobin, tib, ba, fil, elatriye Pou enfòmasyon detaye sou konpozisyon chimik ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan. Imèl: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Tès ak Dokimantasyon: Sètifika tès faktori, EN 10204 3.1, rapò chimik, rapò mekanik, rapò tès destriktif, rapò tès ki pa-destriktif, rapò tès PMI, rapò enspeksyon vizyèl, rapò enspeksyon twazyèm pati, rapò laboratwa sètifye NABL.
Anbalaj: anbalaj kès an bwa, anbalaj vlope jarèt, strapping asye, oswa anbalaj selon kondisyon kliyan.