aisi 321 annealed stainless steel plateWhat is ASTM A240 Type 904L Plates?what is sus316 stainless steel?

 

Q1: Ki sa ki 904L asye pur?

A1: Yon super austenitic Nerjaveèi (UNS N08904) ak gwo Cr (19%), Ni (25%), Mo (4%), ak Cu (2%) -ofri ekselan rezistans korozyon ak bon duktilite.

 

Q2: Kle pwopriyete mekanik (kondisyon rkwit)?

A2: Fòs rupture pi gran pase oswa egal a 520 MPa, fòs sede Pi gran pase oswa egal a 210 MPa, elongasyon pi gran pase oswa egal a 35%, dite mwens pase oswa egal a 220 HB-siperyè duktilite pou fòme / soude.

 

Q3: Ki anviwònman korozivite li reziste?

A3: Reziste asid silfirik, asid fosfò, klori, dlo lanmè, ak asid òganik -ideyal pou kondisyon chimik agresif.

 

Q4: Endistri komen/aplikasyon?

A4: Pwosesis chimik, ekipman pharmaceutique, plant desalination, lwil oliv ak gaz (tuyaux sèvis asid, tiyo, tank).

 

Q5: Ki jan li konpare ak 316L ak 254SMO?

A5: 904L gen pi bon rezistans korozyon pase 316L; 254SMO ofri pi gwo kontni Mo ak rezistans siperyè pitting. 904L se pri-efikas pou anviwònman asid modere-a-grav.