AISI 420 S42000 Nerjaveèi asye fèy fèy ak plak

Jan 22, 2026

Kite yon mesaj

What is 1.4919 Stainless Steel?What is 1.4546 Stainless Steel?What is 1.4571 Stainless Steel?

Estanda

ASTM A176 Standard Spesifikasyon pou Nerjaveèi ak Chalè -Reziste Kwòm Steel Plak, Fèy, ak Strip.

 

Konpozisyon chimik (%)

Klas C Si Mn P S Kr Ni Mo
420 0.15 min 1.0 max 1.0 max 0.040 max 0.030 max 12.0-14.0 0.75 max 0.50 max

Retounen nan tèt

Pwopriyete mekanik

Tanperati Tanperati (degre) Fòs rupture (MPa) Sede fòs

0.2% Prèv (MPa)

Elongasyon (% nan 50mm) Dite Brinell (HB) Enpak Charpy V (J)
rkwit * 655 345 25 241 max –
204 1600 1360 12 444 20
316 1580 1365 14 444 19
427 1620 1420 10 461 #
538 1305 1095 15 375 #
593 1035 810 18 302 22
650 895 680 20 262 42