AISI 347 Nerjaveèi - Premium Niobium Stabilize Klas

Mar 23, 2026

Kite yon mesaj

What is 1.4833 Stainless Steel?What is 1.4845 Stainless Steel?Stainless Steel - Grade 347 - AISI 347 Fe/Cr18/Ni10/Nb (UNS S34700)

🧪 Konpozisyon Chimik

Eleman Konpozisyon (%)
Kabòn (C) Mwens pase oswa egal a 0.08
Manganèz (Mn) Mwens pase oswa egal a 2.00
Silisyòm (Si) Mwens pase oswa egal a 0.75
Fosfò (P) Mwens pase oswa egal a 0.045
Souf (S) Mwens pase oswa egal a 0.030
Kwòm (Cr) 17.0 - 20.0
Nikèl (Ni) 9.0 - 13.0
Niobyòm (Nb) 10 × C min, 1.00 max
Fè (Fe) Balans

⚙️ Pwopriyete mekanik

Pwopriyete Valè
Fòs rupture (tanperati chanm) Pi gran pase oswa egal a 515 MPa
Fòs Sede (0.2% Offset) Pi gran pase oswa egal a 205 MPa
Elongasyon nan 50mm Pi gran pase oswa egal a 40%
Dite (Brinell) Mwens pase oswa egal a 217 HB
Dite (Rockwell B) Mwens pase oswa egal a 95 HRB
Enèji enpak (Charpy V-dan, 20 degre) Pi gran pase oswa egal a 120 J
Limit Fatig (107sik) 240 MPa
Modil Young la 200 GPa

🔬 Pwopriyete Fizik

Pwopriyete Valè
Dansite 7.95 g/cm³
Pwen k ap fonn 1400-1450 degre
Kondiktivite tèmik (20 degre) 14.2 W/m·K
Koefisyan ekspansyon tèmik (20-100 degre) 17.3×10-6/K
Kapasite Chalè Espesifik 500 J/kg·K
Rezistans elektrik (20 degre) 0.73 µΩ·m
Pèmeyabilite mayetik 1.02 (Paramayetik)
Pwopòsyon Poisson a 0.27-0.30

📏 Espesifikasyon pwodwi yo

Fòm pwodwi Gwosè ki disponib Estanda
Plak woule cho Epesè: 6-100mm, Lajè: jiska 2500mm ASTM A240, ASME SA-240
Fèy woule frèt Epesè: 0.4-6mm, Lajè: jiska 1500mm ASTM A240, EN 10088-2
Ba wonn Dyamèt: 6-300mm, Longè: jiska 6000mm ASTM A276, ASTM A479
Tib san pwoblèm OD: 6-610mm, WT: 1-60mm ASTM A213, ASTM A312
Tiyo soude OD: 10-1220mm, WT: 1-40mm ASTM A312, ASTM A358
Fini andigman 2B, BA, No.4, HL, glas ASTM A480
Dimansyon tolerans ± 0.1mm a ± 0.5mm Dapre estanda ASTM yo

Voye rechèch