🧪 Konpozisyon Chimik
| Eleman | Konpozisyon (%) |
|---|---|
| Kabòn (C) | Mwens pase oswa egal a 0.030 |
| Manganèz (Mn) | Mwens pase oswa egal a 2.00 |
| Silisyòm (Si) | Mwens pase oswa egal a 0.75 |
| Fosfò (P) | Mwens pase oswa egal a 0.045 |
| Souf (S) | Mwens pase oswa egal a 0.030 |
| Kwòm (Cr) | 16.00 - 18.00 |
| Nikèl (Ni) | 10.00 - 14.00 |
| Molybdène (Mo) | 2.00 - 3.00 |
| Azòt (N) | Mwens pase oswa egal a 0.10 |
| Fè (Fe) | Balans |
⚙️ Pwopriyete mekanik
| Pwopriyete | Valè |
|---|---|
| Fòs rupture (Rm) | 485 - 620 MPa |
| Fòs Sede (Rp0.2) | Pi gran pase oswa egal a 205 MPa |
| elongasyon (A50mm) | Pi gran pase oswa egal a 40% |
| Dite (HRB) | Mwens pase oswa egal a 95 |
| Dite (HV) | 200 - 250 |
| Enèji enpak (KV) | Pi gran pase oswa egal a 60 J (nan 20 degre) |
| Modil Young la | 200 GPa |
| Limit fatig | 245 MPa (107sik) |
| Pwopòsyon Poisson a | 0.27 - 0.30 |