Lè w ap achte fèy asye pur 904L, konprann epesè, gwosè, ak estanda endistri ki disponib yo enpòtan anpil pou fè bon chwa. Faktè sa yo pa sèlman afekte pri materyèl la, men tou detèmine konvnab pou aplikasyon espesifik, fabrikasyon, ak pèfòmans alontèm-.
Ki estanda pou fèy asye pur 904L?
Plak asye pur 904L (UNS N08904, WNR 1.4539) se yon wo -alyaj asye pur austenitic ak ekselan rezistans korozyon, prensipalman manifaktire dapre ASTM A240 ak EN 10088-2 estanda. Epesè li varye ant 0.3 mm ak plis pase 100 mm (plak woule frèt yo gen 0.3-6 mm epè, ak plak woule cho yo se 3-100 mm epè oswa plis), ak lajè estanda 1000 mm, 1219 mm, ak 1500 mm, ak longè jiska 6000 mm.
| Estanda | Spesifikasyon | Deskripsyon |
|---|---|---|
| ASTM | ASTM A240 / A240M | Estanda pou fèy asye pur ki reziste -chalè ak korozyon- |
| UNS | UNS N08904 | Deziyasyon Sistèm Nimerasyon Inifye pou 904L |
| EN | EN 1.4539 | Ewopeyen estanda ekivalan a 904L |
| JIS | SUS 904L | Estanda Endistriyèl Japonè pou segondè -alyaj asye pur |
| GB | GB/T 20878 | Chinwa estanda pou super austenitic fèy asye pur |
| DIN | DIN 2.4665 | Ekivalan Alman pou fèy ki reziste -kowozyon alyaj segondè |
Epesè fèy asye pur 904L
Fèy asye pur 904L yo disponib nan yon pakèt epesè pou satisfè divès bezwen endistriyèl:
904L Nerjaveèi asye ultra-fèy mens (0.3mm - 1mm): Apwopriye pou eleman presizyon, panno dekoratif, ak ti -fabwikasyon echèl.
904L Nerjaveèi asye Creole fèy (1mm - 6mm): Yo itilize souvan nan tank chimik, kanalizasyon, ak aplikasyon jeneral endistriyèl.
904L Nerjaveèi asye plak epè (6mm - 20mm): Ideyal pou konpozan estriktirèl, gwo -pati maren devwa, ak ekipman presyon wo-.
| Epesè | Gwosè Range | Epesè | Sifas Sifas pou chak pwa inite | Apeprè pwa pou chak fèy | ||
|---|---|---|---|---|---|---|
| pous | mm | kg/m² | liv/pye² | kg | liv | |
| 0.015 | 36 x 120 | 0.381 | 3.07566 | 0.630 | 8.5617 | 18.90 |
| 0.015 | 36 x 96 | 0.381 | 3.07566 | 0.630 | 6.84936 | 15.12 |
| 0.0178 | 36 x 120 | 0.45212 | 3.690792 | 0.756 | 10.27404 | 22.68 |
| 0.0178 | 36 x 96 | 0.45212 | 3.690792 | 0.756 | 8.22195 | 18.15 |
| 0.0178 | 48 x 120 | 0.45212 | 3.690792 | 0.756 | 13.69872 | 30.24 |
| 0.0178 | 48 x 96 | 0.45212 | 3.690792 | 0.756 | 10.95807 | 24.19 |
| 0.0235 | 30 x 120 | 0.5969 | 4.921056 | 1.008 | 11.4156 | 25.20 |
| 0.0235 | 30 x 96 | 0.5969 | 4.921056 | 1.008 | 9.13248 | 20.16 |
| 0.0235 | 36 x 120 | 0.5969 | 4.921056 | 1.008 | 13.69872 | 30.24 |
SA240 904L mezi fèy asye pur
| (Apwoksimatif POUS) | METAL GAUGE | DESIMAL NOMINAL (+/- POUS) |
| 0.1644 | 8 | 0.0080 |
| 0.1793 | 7 | 0.0080 |
| 0.1345 | 10 | 0.0070 |
| 0.1196 | 11 | 0.0050 |
| 0.1495 | 9 | 0.0080 |
| 0.1046 | 12 | 0.0050 |
| 0.0179 | 26 | 0.0015 |
| 0.0747 | 14 | 0.0040 |
| 0.0673 | 15 | 0.0040 |
| 0.0897 | 13 | 0.0050 |
| 0.0598 | 16 | 0.0030 |
| 0.0478 | 18 | 0.0030 |
SS 904L Tablo pwa plak
Fòmil kalkil plak SS 904L

| Nerjaveèi asye 904L Fèy Pwa pou chak fèy (Kg) | Gwosè (mm) | Pwa pou chak fèy (Kg) | Gwosè (mm) |
|---|---|---|---|
| 17.9 | 2500 x1250 x 0.7 | 55.3 | 3000 x 1500 x 1.5 |
| 11.5 | 2000 x1000 x 0.7 | 38.4 | 2500 x 1250 x 1.5 |
| 14.7 | 2000 x1000 x 0.9 | 32.7 | 2000 x 1000 x 2.0 |
| 16.4 | 2000 x1000 x 1.0 | 73.7 | 3000 x 1500 x 2.0 |
| 23.0 | 2500 x1250 x 0.9 | 51.2 | 2500 x 1250 x 2.0 |
| 36.8 | 3000 x1500 x 1.0 | 63.9 | 2500 x 1250 x 2.5 |
| 25.6 | 2500 x1250 x 1.0 | 40.9 | 2000 x 1000 x 2.5 |
| 19.6 | 2000 x1000 x 1.2 | 92.1 | 3000 x 1500 x 2.5 |
| 44.2 | 3000 x1500 x 1.2 | 77.5 | 2500 x 1250 x 3.0 |
| 30.7 | 2500 x1250 x 1.2 | 49.6 | 2000 x 1000 x 3.0 |
| 24.6 | 2000 x1000 x 1.5 | 112.0 | 3000 x 1500 x 3.0 |
904L Nerjaveèi asye Aplikasyon Fèy
| Endistri | Aplikasyon |
|---|---|
| Chimik ak petwochimik | Reaktè, tank, tiyo, echanjeur chalè |
| Marin | Konpozan bato, platfòm lanmè |
| Manje & Bwason | Ekipman pwosesis -wo fen |
| Achitekti | Panno dekoratif, balistrad, fasad |
| Famasetik | Veso depo, sistèm kanalizasyon |
Si ou gen nenpòt kondisyon pou atik ki anwo yo, tanpri ou lib pou mete yon lòd. GNEE gen yon gwo envantè popilè plak asye pur 904L pou ou chwazi nan. Sa yo ka trete nan divès fòm pwodwi pratik. Pou konpozisyon chimik detaye ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan.