440 Nerjaveèi asye plak ak bobin: Ultra - Segondè dite Martensitic Koupe Zouti Plak / Bobin

Jan 30, 2026

Kite yon mesaj

Ki sa ki 440 Nerjaveèi asye plak & bobin?

440 plak asye pur ak bobin se yon wo -kabòn segondè- Kwòm martensitic Nerjaveèi pwodwi, prezante ultra-dite segondè ak rezistans mete apre tretman chalè. Li espesyalize pou koupe zouti, BEARINGS ak gwo -konpozan presizyon mete.

Klas ekivalan (orizontal)

UNS: S44002 (440A) / S44003 (440B) / S44004 (440C)|JIS: SUS440A/B/C|GB: 8Cr17 (440A)|EN: X90Cr18 (440C)|W.Nr.: 1.4028 (440A)

Konpozisyon chimik (pwa%, orizontal, 440C)

C: 0.95-1.20|Si: Mwens pase oswa egal a 1.00|Mn: Mwens pase oswa egal a 1.00|P: Mwens pase oswa egal a 0.040|S: Mwens pase oswa egal a 0.030|Cr: 16.00-18.00|Mo: 0.75-1.25|Fe: Balans

Pwopriyete kle (20 degre, trempe ak tanperaman, orizontal)

Dansite: 7.75g/cm³|Pwen k ap fonn: 1450-1510 degre|Fòs Tensile: Pi gran pase oswa egal a 735N/mm²|Fòs Sede: Pi gwo pase oswa egal a 540N/mm²|Elongasyon: Pi gran pase oswa egal a 10%|Dite: Pi gran pase oswa egal a 58HRC

Karakteristik debaz yo

• Ultra -segondè dite: Apre trempe ak tanperaman, dite rive nan 58-62HRC, ak rezistans mete eksepsyonèl • Gwo rezistans korozyon: kontni segondè Kwòm amelyore rezistans nan medya korozivite twò grav, apwopriye pou kondisyon travay difisil • Estabilite dimansyon bon: Ba deformation pandan tretman chalè, asire zouti segondè presizyon ak konpozan koupe: Aplike nan zouti pou koupe, BEARINGS, tiyo ak gwo -presizyon pati ki reziste

440C vs 420 Nerjaveèi asye plak ak bobin (orizontal)

C Kontni: 440C (0.95-1.20%)|420 (0.16-0.25%)|Dite: 440C (ultra-wo)|420 (Segondè)|Mete Rezistans: 440C (Siperyè)|420 (Ekselan)|Machinability: 440C (Pòv)|420 (pi bon)

 

Founisè asye pur

Si ou gen kondisyon pwojè pou asye pur, nou akeyi lòd ou a. GNEE gen yon gwo envantè de pwodwi popilè pou ou pou w chwazi. Li ka trete nan divès fòm pwodwi pratik, ki gen ladan plak, bobin, tib, ba, fil, elatriye Pou enfòmasyon detaye sou konpozisyon chimik ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan. Imèl: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Tès ak Dokimantasyon: Sètifika tès faktori, EN 10204 3.1, rapò chimik, rapò mekanik, rapò tès destriktif, rapò tès ki pa-destriktif, rapò tès PMI, rapò enspeksyon vizyèl, rapò enspeksyon twazyèm pati, rapò laboratwa sètifye NABL.
Anbalaj: anbalaj kès an bwa, anbalaj vlope jarèt, strapping asye, oswa anbalaj selon kondisyon kliyan.