🧪 Konpozisyon Chimik
Konpozisyon chimik:
| Eleman | % min | Max % | % tipik | Egzijans ASTM A276 |
|---|---|---|---|---|
| Kabòn (C) | - | 0.080 | 0.035 | Mwens pase oswa egal a 0.08 |
| Kwòm (Cr) | 16.0 | 18.0 | 17.2 | 16.0-18.0 |
| Nikèl (Ni) | 10.0 | 14.0 | 12.0 | 10.0-14.0 |
| Molybdène (Mo) | 2.0 | 3.0 | 2.3 | 2.0-3.0 |
| Manganèz (Mn) | - | 2.00 | 1.35 | Mwens pase oswa egal a 2.00 |
| Silisyòm (Si) | - | 0.75 | 0.38 | Mwens pase oswa egal a 0.75 |
| Fosfò (P) | - | 0.045 | 0.025 | Mwens pase oswa egal a 0.045 |
| Souf (S) | - | 0.030 | 0.012 | Mwens pase oswa egal a 0.030 |
| Azòt (N) | - | 0.10 | 0.05 | Mwens pase oswa egal a 0.10 |
| Fè (Fe) | Balans | Balans | 66.1 | Balans |
⚙️ Pwopriyete mekanik
Pwopriyete mekanik:
| Pwopriyete | Egzijans ASTM | Valè tipik | Metòd tès | Tanperati |
|---|---|---|---|---|
| Fòs rupture | 515 MPa min | 620 MPa | ASTM A370 | Tanperati chanm |
| Fòs Sede (0.2%) | 205 MPa min | 310 MPa | ASTM A370 | Tanperati chanm |
| Elongasyon | 30% min | 40% | ASTM A370 | Tanperati chanm |
| Dite (Brinell) | 217 HB max | 185 HB | ASTM E10 | Tanperati chanm |
| Dite (Rockwell B) | 95 HRB max | 88 HRB | ASTM E18 | Tanperati chanm |
| Modil Elastisite | - | 200 GPa | ASTM E111 | Tanperati chanm |
| Enèji enpak (Charpy V) | - | 325+ J | ASTM E23 | Tanperati chanm |