316 Nerjaveèi asye plak se yon asye pur austenitic

Apr 14, 2026

Kite yon mesaj

SUS304 Austenitic Stainless Steel – Versatile Corrosion-Resistant Universal Alloy304 Stainless Steel Round Bar from GneeSUS304L Austenitic Stainless Steel – Low-Carbon Weld-Stable Corrosion SolutionSUS316 Austenitic Stainless Steel – Molybdenum-Enhanced Chloride-Resistant Alloy

Regleman biznis

Regleman Spesifikasyon
Kantite minimòm lòd: 5 tòn
Pri: Pou negosye
Detay anbalaj:

Jan yo mande

Tan livrezon: Nan 7-10 jou travay
Kondisyon Peman: T/T, L/C, Kat kredi
Kapasite Pwovizyon pou: 100000 Tòn pa mwa
Sètifikasyon: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Ekspòte pou:

Etazini, Wayòm Ini, Ostrali, peyi Zend, Kore di, Hong Kong, Federasyon Larisi, Brezil, Malezi, Kanada, FilipinEtazini, Endonezi, pèp Izrayèl la, Afganistan, Albani, Aljeri, Samoa Ameriken, Andorra, Angola, AnguillaAntigwa ak Barbuda, Ajantin, Ameni, Otrich, Azerbaydjan, Bahamas, Bahrain, Bangladès, Bèlji, Bèlji, Bèlji, Bèlji, Bèli elatriye.

Konpozisyon chimik

Eleman Kabòn (C) Kwòm (Cr) Nikèl (Ni) Manganèz (Mn) Silisyòm (Si) Fosfò (P) Souf (S) Molybdène (Mo) Azòt (N) Fè (Fe)
                     
Range 0.08 max 16.0 – 18.0 10.0 – 14.0 2.0 max 1.0 max 0.045 max 0.03 max 2.0 – 3.0 0.10 max Balans

Pwopriyete mekanik

Pwopriyete Inite metrik Inite Imperial
     
Fòs rupture 515 - 690 MPa 74,700 - 100,000 psi
Sede fòs 205 MPa 30,000 psi
Vickers dite 150 - 220 HV 150 - 220 HV
Brinell dite 146 – 217 HB 146 – 217 HB
Rockwell dite B80 – B95 B80 – B95
Elongasyon 40% 40%
Modil elastik 193 - 200 GPa 28,000 - 29,000 ksi

Tretman Chalè

Sheet Plate Heat Treatment

Recuit

Tanperati: 1,040 - 1,120 degre (1,900 - 2,050 degre F)

Pwosesis: Chofe ak Lè sa a, rapidman refwadi, tipikman pa lè oswa dlo asouvisman

Soulaje estrès

Tanperati: 450 - 600 degre (840 - 1,110 degre F)

Pwosesis: Chofe epi ki te swiv pa lè refwadisman

Redi

Mwens komen

316 asye pur pa ka fè tèt di pa tretman chalè, sèlman pa travay frèt

Tretman solisyon

Tanperati: 1,010 - 1,120 degre (1,850 - 2,050 degre F)

Pwosesis: Chofe ak etenn pou fonn presipite ak amelyore rezistans korozyon