STANDARD UNS WNR. AFNOR EN JIS BS GOST
SS 304 S30400 1.4301 Z7CN18-09 X5CrNi18-10 SUS 304 304S31 08Х18Н10
SS 304L S30403 1.4306/1.4307 Z3CN18‐10 X2CrNi18-9 / X2CrNi19-11 SUS 304L 304S11 03Х18Н11
SS 304H S30409 1.4301 - - - - -

Konpozisyon chimik nan Nerjaveèi 304/304L/304H Tiyo & Tib

  C Mn Si P S Kr Ni N
304 0.07 max 2.0max 0.75 max 0.045 max 0.03max min: 18.0 max: 20.0 min: 8.0 max: 10.5 -
304L 0.03max 2.0max 0.75 max 0.045 max 0.03max min: 18.0 max: 20.0 min: 8.0 max: 12.0 0.10 max
304H min: 18.0
maksimòm: 20.0
min: 8.0
maksimòm: 10.5
min: 0.04
maksimòm: 0.10
0.75
max
2.0
max
0.045
max
0.03
max
0.10
max

Pwopriyete mekanik nan asye pur 304/304L/304H Tiyo & Tib

Klas Fòs Tensile ksi (min) Sede fòs 0.2% ksi (min) Elongasyon % Dite (Brinell) MAX Dite (Rockwell B) MAX
304 75 30 40 201 92
304L 70 25 40 201 92
304H 75 30 40 201 92