304L Stainless Steel Pipe for Nuclear Power Auxiliary SystemsUNS S30908 Stainless Steel – High-Chromium Heat-Resistant Utility Alloy304L Stainless Steel Sheet for Chemical Tank Linings

 

Pwopriyete Fizik

Pwopriyete fizik asye pur AISI 304L yo bay nan lis sa yo, ki gen ladan dansite, pwen k ap fonn ak pèmeyabilite mayetik.

SS304L Pwopriyete Fizik
Dansite, g/cm3 (lb/in.3) 8.03 (0.29)
Pwen k ap fonn, degre (degre F) 1400-1450 (2550-2650)
Pèmeyabilite mayetik 1.02 (Apwoksimatif)

Pwopriyete mekanik

304 vs 304L Nerjaveèi asye mekanik pwopriyete nan tanperati chanm yo ki nan lis nan tablo sa yo.

304 vs 304L Pwopriyete mekanik
ASTM Kalite AISI Kondisyon yo Fòs Tensile, MPa (ksi), Pi gran pase oswa egal a 0.2% Sede Fòs, MPa (ksi), Pi gran pase oswa egal a Elongasyon nan 50 mm (2 pous), %, Pi gran pase oswa egal a Rediksyon nan zòn, %, pi gran pase oswa egal a Brinell dite (HBW), mwens pase oswa egal a Rockwell Hardness (HRBW), Mwens pase oswa egal a Fòm pwodwi
ASTM A276/A276M 304 Rekwit, cho fini 515 (75) 205 (30) 40 50 – – Ba ak fòm
304L 485 (70) 170 (25) 40 50 – –
304 Rekwit, fini frèt, Diamètre mwens pase oswa egal a 12.7 mm (0.5 pous) 620 (90) 310 (45) 30 40 – –
304L
304 Rekwit, fini frèt, Diamèt > 12.7 mm (0.5 pous) 515 (75) 205 (30) 30 40 – –
304L 485 (70) 170 (25) 30 40 – –
ASTM A580/A580M 304 Rkwit 520 (75) 210 (30) 35 50     Fil
304L 485 (70) 170 (25) 35 50 – –
304 Fwad fini 620 (90) 310 (45) 30 40 – –
304L
ASTM A240/A240M 304   515 (75) 205 (30) 40 – 201 92 Plak, Fèy, ak bann
304L   485 (70) 170 (25) 40 – 201 92
ASTM A473/A473M 304 Rekwit, Seksyon ki mwens pase oswa egal a 5 pous (127 mm) 515 (75) 205 (30) 40 50 – – Forgings
Rekwit, Seksyon > 5 pous (127 mm) 70 (485)
304L   450 (65) 170 (25) 40 50 – –