Ki sa ki 304H Nerjaveèi asye tiyo & Tib?
304H Nerjaveèi asye tiyo & Tib se varyant segondè-kabòn seri 304, espesyalman fòmile pou amelyore fòs ranpe tanperati ki wo -. Li fèt pou gwo -tanperati, gwo -estrès aplikasyon pou kanalizasyon tankou surchofaj chofaj ak tib endistriyèl gwo founo dife.
Klas ekivalan (orizontal)
UNS: S30409|JIS: SUS304H|GB: 07Cr19Ni10|EN: X6CrNi18-10|W.Nr.: 1.4307
Konpozisyon chimik (pwès%, orizontal)
C: 0.04-0.10|Si: Mwens pase oswa egal a 1.00|Mn: Mwens pase oswa egal a 2.00|P: Mwens pase oswa egal a 0.045|S: Mwens pase oswa egal a 0.030|Cr: 18.00-20.00|Ni: 8.00-10.50|N: Mwens pase oswa egal a 0.10|Fe: Balans
Pwopriyete kle (20 degre, rkwit, orizontal)
Dansite: 7.93g/cm³|Pwen k ap fonn: 1400-1450 degre|Fòs Tensile: Pi gwo pase oswa egal a 515N/mm²|Fòs Sede: Pi gwo pase oswa egal a 205N/mm²|Elongasyon: Pi gran pase oswa egal a 40%|Dite: Mwens pase oswa egal a 201HB
Karakteristik debaz yo
• Segondè kontni kabòn: Siyifikativman amelyore gwo -tanperati ranpe fòs, kenbe entegrite estriktirèl anba 600-870 degre-estrès alontèm • Bon segondè-rezistans oksidasyon tanperati, apwopriye pou sèvis kontinyèl segondè-tanperati nan atmosfè oksidan • Pòs obligatwa ak estrikti inifòm: pèfòmans tanperati ki wo -, evite diminisyon pèfòmans • Ideyal pou gwo -tanperati, konpozan tiyo segondè presyon nan plant elektrik, chodyèr ak gwo founo endistriyèl.
304 vs 304H Nerjaveèi asye Tiyo & Tib (Orizontal)
Kontni Kabòn: 304 (mwens pase oswa egal a 0.08%)|304H (0.04-0.10%)|Gwo -Fòs Flux Tanperati: 304 (Jeneral)|304H (Ekselan)|Recuit: 304 (Si ou vle)|304H (Obligatwa)|Adaptabilite segondè-tanperati: 304 (mwens pase oswa egal a 800 degre)|304H (mwens pase oswa egal a 870 degre)
| Klas | UNS No. | EN Non. | C | Kr | Ni | Mo | Lòt moun |
| 304 | S30400 | 1.4301 | 0.08 | 18.00 - 20.00 | 8.00 - 12.00 | - | - |
| 304L | S30403 | 1.4307 | 0.035 | 18.00 - 20.00 | 8.00 - 12.00 | - | - |
| 310S | S31008 | 1.4845 | 0.08 | 24.00 - 26.00 | 19.00 - 22.00 | - | - |
| 316 | S31620 | 1.4401 | 0.08 | 16.00 - 18.00 | 10.00 - 14.00 | 2.00 - 3.00 | - |
| 316L | S31603 | 1.4404 | 0.035 | 16.00 - 18.00 | 10.00 - 14.00 | 2.00 - 3.00 | - |
| 316H | S31603 | - | 0.04 - 0.10 | 16.00 - 18.00 | 10.00 - 14.00 | 2.00 - 3.00 | - |
| 316Ti | S31635 | 1.4571 | 0.08 | 16.00 - 18.00 | 10.00 - 14.00 | 2.00 - 3.00 | Ti:5X(C+N) - 0.70 |
| 317L | S31703 | 1.4438 | 0.035 | 18.00 - 20.00 | 11.00 - 15.00 | 3.00 - 4.00 | - |
| 321 | S32100 | 1.4541 | 0.08 | 17.00 - 19.00 | 9.00 - 12.00 | - | Ti:5X(C+N) - 0.70 |
| 347 | S34700 | 1.4550 | 0.08 | 16.00 - 18.00 | 10.00 - 14.00 | - | - |
| 347H | S34709 | 1.4551 | 0.04 - 0.10 | 17.00 - 20.00 | 9.00 - 13.00 | - | - |
| 904L | S8904 | 1.4539 | 0.02 | 19.00 - 23.00 | 23.00 - 28.00 | - | N: 0.10 max Cu : 1.0 - 2.0 |
304 Founisè Nerjaveèi
Si ou gen kondisyon pwojè pou 304 asye pur, nou akeyi lòd ou a. GNEE gen yon gwo envantè de pwodwi popilè pou ou pou w chwazi. Li ka trete nan divès fòm pwodwi pratik, ki gen ladan plak, bobin, tib, ba, fil, elatriye Pou enfòmasyon detaye sou konpozisyon chimik ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan. Imèl: info@gneestainless.com



Tès ak Dokimantasyon: Sètifika tès faktori, EN 10204 3.1, rapò chimik, rapò mekanik, rapò tès destriktif, rapò tès ki pa-destriktif, rapò tès PMI, rapò enspeksyon vizyèl, rapò enspeksyon twazyèm pati, rapò laboratwa sètifye NABL.
Anbalaj: anbalaj kès an bwa, anbalaj vlope jarèt, strapping asye, oswa anbalaj selon kondisyon kliyan.


Voye rechèch