304 plak seri asye pur yo se asye pur austenitic
Apr 14, 2026
Kite yon mesaj




Kondisyon biznis pwodwi
| Regleman biznis | Espesifikasyon |
|---|---|
| Kantite minimòm lòd: | 5 tòn |
| Pri: | Pou negosye |
| Detay anbalaj: |
Jan yo mande |
| Tan livrezon: | Nan 7-10 jou travay |
| Kondisyon Peman: | T/T, L/C, Kat kredi |
| Kapasite Pwovizyon pou: | 100000 Tòn pa mwa |
| Sètifikasyon: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Ekspòte pou: |
Etazini, Kanada, Filipin, peyi Zend, Ostrali, Wayòm Ini, Malezi, Federasyon Larisi, Endonezi, Meksik, Brezil, Almay, Kore di, Thailand, Emira Arab Ini, Vyetnam, Lafrans, Hong Kong, Itali, Netherlands, New Zeland, Singapore, Espay, Taiwan, Ajantin, Bangladèch, Kanbòdj, Fenlann, Lagrès, Nijerya, Pakistan, Katar, Arabi Saoudit, Turkey, elatriye. |
Konpozisyon chimik
| Klas | Kwòm (Cr) | Nikèl (Ni) | Kabòn (C) | Manganèz (Mn) | Silisyòm (Si) | Fosfò (P) | Souf (S) |
|---|
| 304 | 18.0-20.0% | 8.0-10.5% | Mwens pase oswa egal a 0.08% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
| 304L | 18.0-20.0% | 8.0-12.0% | Mwens pase oswa egal a 0.03% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
| 304H | 18.0-20.0% | 8.0-12.0% | Mwens pase oswa egal a 0.04% | Mwens pase oswa egal a 2.0% | Mwens pase oswa egal a 1.0% | Mwens pase oswa egal a 0.045% | Mwens pase oswa egal a 0.03% |
Pwopriyete mekanik
| Pwopriyete | 304 | 304L | 304H |
|---|
| Fòs rupture | 515 - 750 MPa (75 - 108.8 ksi) | 485 - 700 MPa (70 - 101.5 ksi) | 515 - 750 MPa (75 - 108.8 ksi) |
| Sede fòs | 205 MPa (30 ksi) | 170 MPa (25 ksi) | 275 MPa (40 ksi) |
| Dite Brinell (HBW) | 123 – 201 | 123 – 201 | 123 – 201 |
| Rockwell Hardness (HRB) | 70 – 90 | 70 – 90 | 70 – 90 |
| Vickers dite (HV) | 129 – 210 | 129 – 210 | 129 – 210 |
| Allongement nan Break | 40% | 40% | 40% |
| Modil Young la | 193 - 200 GPa (28 - 29 msi) | 193 - 200 GPa (28 - 29 msi) | 193 - 200 GPa (28 - 29 msi) |