Konpozisyon chimik:

Eleman % min Max % % tipik Egzijans ASTM A276
Kabòn (C) - 0.080 0.045 Mwens pase oswa egal a 0.08
Kwòm (Cr) 18.0 20.0 18.5 18.0-20.0
Nikèl (Ni) 8.0 12.0 9.2 8.0-12.0
Manganèz (Mn) - 2.00 1.45 Mwens pase oswa egal a 2.00
Silisyòm (Si) - 0.75 0.42 Mwens pase oswa egal a 0.75
Fosfò (P) - 0.045 0.028 Mwens pase oswa egal a 0.045
Souf (S) - 0.030 0.015 Mwens pase oswa egal a 0.030
Azòt (N) - 0.10 0.06 Mwens pase oswa egal a 0.10
Fè (Fe) Balans Balans 70.1 Balans

⚙️ Pwopriyete mekanik

Pwopriyete mekanik:

Pwopriyete Egzijans ASTM Valè tipik Metòd tès Tanperati
Fòs rupture 515 MPa min 620 MPa ASTM A370 Tanperati chanm
Fòs Sede (0.2%) 205 MPa min 310 MPa ASTM A370 Tanperati chanm
Elongasyon 40% min 50% ASTM A370 Tanperati chanm
Dite (Brinell) 201 HB max 180 HB ASTM E10 Tanperati chanm
Dite (Rockwell B) 92 HRB max 88 HRB ASTM E18 Tanperati chanm
Modil Elastisite - 200 GPa ASTM E111 Tanperati chanm
Enèji enpak (Charpy V) - 325+ J ASTM E23 Tanperati chanm