Kalite 304 klas asye pur konpozisyon yo bay nan tablo ki anba a.
Datasheet 1, AISI 304 konpozisyon asye pur
| Konpozisyon chimik, % | ||||||||||
| ASTM | AISI (UNS) | C, mwens pase oswa egal a | Si, mwens pase oswa egal a | Mn, Mwens pase oswa egal a | P, mwens pase oswa egal a | S, mwens pase oswa egal a | Kr | Ni | N, mwens pase oswa egal a | Pwodwi |
| ASTM A240/A240M | 304 (UNS S30400) | 0.07 | 0.75 | 2.00 | 0.045 | 0.030 | 17.5-19.5 | 8.0-10.5 | 0.10 | Plak, Fèy, ak bann |
| ASTM A276/276M | 0.08 | 1.00 | 2.00 | 0.045 | 0.030 | 18.0-20.0 | 8.0-11.0 | – | Ba ak fòm | |
SS304 Nerjaveèi asye mekanik pwopriyete
Datasheet-2, tablo ki anba yo lis pwopriyete mekanik materyèl SS304 ki gen ladan fòs sede, fòs rupture, elongasyon ak dite, elatriye.
| Pwopriyete mekanik, done yo se pou 25.4 mm (1 pous) ba dyamèt | ||||||
| Steel (UNS) | Fòs rupture, MPa (ksi) | Fòs sede, MPa (ksi) | Elongasyon nan 50 mm (2 pous), % pi gran pase oswa egal a | Rediksyon nan zòn (%) | Dite (HB) | Kondisyon |
| AISI 304 (UNS S30400) | 585 (85) | 235 (34) | 60 | 70 | 149 | Ba rkwit |
| 690 (100) | 415 (60) | 45 | 212 | Rekwit ak frèt trase | ||
| 860 (125) | 655 (95) | 25 | 275 | Fwad trase segondè tansyon | ||
Datasheet 3, ASTM 304 Pwopriyete Nerjaveèi - Pwopriyete mekanik
| Pwopriyete mekanik | |||||||||
| Kalite ASTM | AISI (UNS) | Fòs rupture, MPa (ksi) | 0.2% Sede fòs, MPa (ksi) | Elongasyon nan 50 mm (2 pous), % pi gran pase oswa egal a | Rediksyon nan zòn, %, pi gran pase oswa egal a | Dite Brinell (HBW) Mwens pase oswa egal a | Rockwell Hardness (HRBW) Mwens pase oswa egal a | Pwodwi | Kondisyon |
| ASTM A240/A240M | 304 (UNS S30400) | 515 (75) | 205 (30) | 40 | – | 201 | 92 | Plak, Fèy, ak bann | – |
| ASTM A276A/276M | 515 (75) | 205 (30) | 40 | 50 | – | – | Ba ak fòm | Cho fini | |
| 620 (90) | 310 (45) | 30 | 40 | – | – | Fwad fini, Dia mwens pase oswa egal a 12.7mm (0.5 pous) | |||
| 515 (75) | 205 (30) | 30 | 40 | – | – | Frèt fini, Dia. > 12.7mm (0.5 pous) | |||