201 Fèy asye pur pou kliyan
Mar 16, 2026
Kite yon mesaj



| Estanda | ASTM A240, EN 10088-2, GB/T 3280 |
|---|---|
| Klas | 1.4372, SUS201, X12CrMnNiN17-7-5, Z12CMN17-07Az |
| Longè | 2000 mm-6000 mm (78.74-236.22 nan), Customized |
| Tout Lajè | 1000 mm-2000 mm (39.37-78.74 nan), Customized |
| Epesè | 0.3 mm-6 mm (0.012-0.24 nan), Customized |
| Sifas fini | 2B, 8K, BA, elatriye, HL, No.1, No.4 |
| Teknik | Fwad trase, frèt woule, cho woule |
| Fòm | Bobin, fèy woule frèt, fèy relief, elatriye, plak plat ak fèy, fèy woule cho, fèy pèse, plak, fèy poli, teren, fèy papye teksti. |
Konpozisyon chimik
| Eleman | Kabòn (C) | Manganèz (Mn) | Silisyòm (Si) | Fosfò (P) | Souf (S) | Kwòm (Cr) | Nikèl (Ni) | Azòt (N) |
|---|
| Konpozisyon (%) | 0.15 max | 5.5-7.5 | 1.0 max | 0.06 max | 0.03 max | 16.0-18.0 | 3.5-5.5 | 0.25 max |
Pwopriyete mekanik
| Pwopriyete | Inite metrik | Inite Imperial |
|---|
| Fòs rupture | 655 – 860 MPa | 95 – 125 ksi |
| Sede fòs | 450 MPa | 65 ksi |
| Vickers dite | 230 - 270 HV | 230 - 270 HV |
| Brinell dite | 200 - 250 HB | 200 - 250 HB |
| Rockwell dite | 50 - 56 HRC | 50 - 56 HRC |
| Elongasyon | 20% | 20% |
| Modil elastik | 200 GPa | 29 x 10^6 psi |
Voye rechèch