17-7PH Nerjaveèi asye fèy, FOIL & retire rad sou ou nan Lachin

Apr 14, 2026

Kite yon mesaj

Stainless Steels - Introduction To The Grades And FamiliesWhat is 1.4568 stainless steel equivalent to?What is 1.4532 Stainless Steel?Seamless Pipe in Avesta 254SMO S31254 DIN1.4547 10 SCH10 Stainless Steel Tube

Regleman biznis

ReglemanSpesifikasyon
Kantite minimòm lòd:5 tòn
Pri:Pou negosye
Detay anbalaj:

Jan yo mande

Tan livrezon:Nan 7-10 jou travay
Kondisyon Peman:T/T, L/C, Kat kredi
Kapasite Pwovizyon pou:100000 Tòn pa mwa
Sètifikasyon:RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Ekspòte pou:

Etazini, Kore di, Taiwan, Almay, Japon, Lafrans, peyi Zend, Wayòm Ini, Federasyon Larisi, Kanada, Brezil, Turkey, Netherlands, Itali, Malezi, Espay, Polòy, Ostrali, Thailand, Bangladèch, Cote D'Ivoire, Denmark, Fidji, Hong Kong, Meksik, Filipin, Syèd, Turkey, Uganda, elatriye.

Konpozisyon chimik

ElemanCMnSiKrNiAlPS
         
Kontni≤0.09≤1.00≤1.0016.0-18.06.5-7.750.75-1.50≤0.04≤0.03

Pwopriyete mekanik

PwopriyeteInite metrikInite Imperial
   
Fòs rupture490 - 690 MPa71 – 100 ksi
Sede fòs≥ 220 MPa≥ 32 ksi
Vickers dite160 - 190 HV160 - 190 HV
Brinell dite≤ 210 HB≤ 210 HB
Rockwell diteB92 maxB92 max
Elongasyon≥ 35%≥ 35%
Modil elastik190 - 210 GPa27.6 – 30.4 × 10³ ksi