15-5PH Founisè Nerjaveèi|Aerospace Klas Bar, Plak ak Solisyon Fèy

Mar 10, 2026

Kite yon mesaj

GNEE offers a stable supply of 15-5PH (UNS S15500) precipitation-hardening stainless steel in the form of bars (06–300 mm) and plates/sheets (0.5–80 mm thick), all compliant with ASTM A564/A693 standards. Products are available in a full range of solution-annealed and aged conditions (such as H900, H1025, and H1150); following precipitation hardening, they achieve a tensile strength (Rm) of up to >1310 MPa ak yon fòs sede (Rp0.2) ki pi gran pase oswa egal a 1170 MPa. Tout liy pwodwi sibi 100% tès ultrasons (satisfè klas AAA estanda).

15-5PH Stainless Steel Round bar
15-5PH Nerjaveèi asye wonn ba
15-5PH Stainless Steel Plate
15-5PH Nerjaveèi asye plak
15-5PH Stainless Steel PMI
15-5PH Nerjaveèi PMI

Nou bay sèvis -koupe sou demann ak tolerans dimansyon jisteman kontwole nan ±0.05 mm, epi bay sètifika kalite EN 10204 3.1 ki detaye konpozisyon chimik konplè ak rezilta tès pwopriyete mekanik.

 

Nòt fabrikasyon ak tretman chalè

Solisyon Anneal: 1,900 - 1,950 degre F (1,040 - 1,065 degre), dlo pasè → mou, mayetik, machinable.

Aje: 900 - 1,150 degre F (480 - 620 degre), 2-4 èdtan, lè fre → presipite redi.

Machining: Pi bon fè nan kondisyon rkwit (A); H900+ mande pou carbure oswa HSS ak alimentation ki ba.

Soude: Difisil nan kondisyon fè tèt di toujou; soude nan rkwit, apresa re-asanble konplè a.

Fòme: Fèy / plak fòme nan kondisyon A oswa H1150 (pi mou), Lè sa a, ki gen laj apre fòme.

Enspeksyon: Aerospace-klas (AMS 5659 Tip 1/2) mande pou yon enspeksyon konplè radyografi + mayetik patikil pou chak ba.

 

15-5PH Nerjaveèi Creole

Fòm ASTM ASME AMS Lòt
Bar A564 / A484 SA-564 AMS 5659 BMS 7-240, STD 2154
Plak / Fèy / Dezabiye A693 / A698 / A705 SA-693 / SA-705 AMS 5862 BMS 7-240, GE S400
Metrik (EN) - - - 1.4545 (X4CrNiCuNb16-4)

 

15-5PH Nerjaveèi asye konpozisyon chimik

Eleman Ranje (%)
Kabòn Mwens pase oswa egal a 0.07
Kwòm 14.00 – 15.50
Nikèl 3.50 – 5.50
Kwiv 2.50 – 4.50
Nb + Ta 0.15 – 0.45
Manganèz Mwens pase oswa egal a 1.00
Silisyòm Mwens pase oswa egal a 1.00

 

15-5PH Nerjaveèi asye mekanik pwopriyete pa kondisyon tretman chalè

Kondisyon UTS (ksi) 0.2% Sede (ksi) elongasyon (%) Dite (HRC)
A (rekuit) 150 110 8–15 Mwens pase oswa egal a 33
H900 (900 degre F / 482 degre) 190 170 10–15 40–47
H925 170 155 10 38–45
H1025 155 145 12 35–42
H1075 145 125 13 33–39
H1100 140 115 14 32–38
H1150 135 105 15–16 28–37
H1150M (Modifye) 135 105 15 28–37

 

15-5PH Nerjaveèi asye gwosè chenn pa fòm

Fòm Gamme tipik Nòt
Bar wonn ⅛" - 6.5" (3 - 165 mm) dia. AMS 5659; VAR oswa ESR fonn
Kare / Egzagòn Bar ¼" - 4" (6 - 100 mm)  
Flat Bar ⅛" - 2" epè × ⅜" - 12" lajè  
Plak 3/16" - 4" (5 - 100 mm) epè ASTM A693; lajè jiska 120"
Fèy / retire rad sou ou 0.025" - 0.250" (0.6 - 6.3 mm) AMS 5862; 2D oswa BA fini; lajè a 48"

 

15-5PH Nerjaveèi asye pwopriyete fizik

Pwopriyete Valè
Dansite 0.280 – 0.284 lb/in³ (7.75 – 7.86 g/cm³)
Ranje k ap fonn 2,510 - 2,550 degre F (1,375 - 1,395 degre)
Kondiktivite tèmik (70 degre F) ~10.6 Btu/hr·ft· degre F (18 W/m·K)
Rezistivite elektrik 77 – 98 μΩ·pous
Mayetik Wi (tout kondisyon)

 

15-5PH Nerjaveèi aplikasyon pou

Endistri Eleman
Aerospace Pati Kovèti pou aterisaj, mòn motè, broch actuator, fixation, ekipman estriktirèl, lam turbine
Nikleyè / pouvwa Entèn reyaktè, konpozan kenbe, arbr turbine
Lwil oliv ak gaz Zouti pou twou, kò valv, arbr ponp, ekipman pou tèt pi (H₂S reziste)
Marin / Offshore Arbr elis, gréement bò rivaj, fixation ki gen gwo -fòs
Jeneral Endistriyèl Kovèti pou, mouri bòdi, kaka ak ekipman papye, arbr pwosesis manje

 

FAQ

K: Ki diferans ki genyen egzakteman ant 15-5PH ak 17-4PH?
15-5PH se yon "vèsyon modènize" 17-4PH. 15-5PH ki pwodui lè l sèvi avèk pwosesis **Vacuum Arc Remelting (VAR) oswa Electroslag Remelting (ESR)**, sa ki lakòz pite materyèl ki pi wo ak yon mikwostrikti nòmalman san ferit; li se tipikman 15%-30% pi chè pase 17-4PH.
17-4PH gen relativman pòv transverse (radial) severite. Si w ap fabrike gwo pati ki dwe kenbe tèt ak gwo chaj transverse (tankou gwo ponp ponp oswa konpozan estriktirèl avyon), ou dwe chwazi 15-5PH akòz izotropi ekselan li yo.


K: Èske 15-5PH ka ranplase 316L?
Se pa yon ranplasan dirèk.
Fòs: 15-5PH se 3 a 4 fwa pi fò pase 316L.
Rezistans korozyon: Rezistans korozyon nan 15-5PH se konparab ak 304 men enferyè a 316L (espesyalman nan anviwònman maren ki gen iyon klori).
Konklizyon: Chwazi 15-5PH si ou bezwen gwo fòs ak dite; chwazi 316L oswa super duplex Nerjaveèi si ou bezwen siperyè rouye ak rezistans korozyon.


K: Èske 15-5PH difisil pou machin?
A: machinabilite li yo sanble ak sa yo ki an 304 asye pur. Piske li gen tandans fè travay -di, li rekòmande pou itilize zouti carbure ki gen gwo dite -e kenbe koupe kontinyèl.


K: Èske 15-5PH mande pou prechofaj pou soude?
A: Anjeneral, non.
Kontrèman ak estanda asye pur martensitic, 15-5PH gen yon kontni kabòn ki ba anpil, ki fè li mwens sansib a fann soude.
Sepandan, sonje ke pou reyalize fòs ekivalan a metal debaz la, yon tretman chalè konplè (re-tretman solisyon ki te swiv pa aje) nesesè apre soude.


K: Poukisa pati ayewospasyal yo souvan mande pou konfòmite AMS 5659?

A: AMS 5659 se estanda klas -ayewospasyal pou ba 15-5PH ak forging. Li mande ke materyèl la dwe pwodui lè l sèvi avèk pwosesis VAR (Vacuum Arc Remelting). Si kliyan ou espesifye estanda AMS la, estanda ASTM A564 materyèl pa ka satisfè kondisyon pou pite materyèl ak tès ultrasons.

 

K: Èske materyèl sa a nan stock? Ki tan tipik nan plon?
A: Round Bar: Stock se abondan, espesyalman pou espesifikasyon satisfè AMS 5659 oswa ASTM A564.
Plak: Stock relativman limite; gwo gwosè ka mande pou yon lòd koutim soti nan moulen an.
Forgings: Tipikman mande pou yon tan plon 4-6 semèn pou pwodiksyon koutim.