Lè w ap chwazi asye pur pou anviwònman trè korozivite oswa segondè-presyon, chwazi ant1.4462ak1.4410Klas duplex ka siyifikativman enpak pèfòmans ak depans lifecycle . tou de ofri rezistans kowozyon eksepsyonèl ak fòs mekanik, men yo diferan nan kontni alyaj, ranje pèfòmans, ak pri .

 

Èske 1.4410 super duplex?

1.4410 stainless steel, also known as X2CrNiMoN25-7-4, is a super duplex stainless steel commonly referred to as Super Duplex 2507 or UNS S32750. It contains 25% chromium, 7% nickel, and 4% molybdenum, offering extremely high resistance to chloride stress corrosion cracking, pitting, and Crevice korozyon . fòs rendement li yo se plis pase de fwa sa yo ki an 316L, epi li lajman ki itilize nan tribin lanmè, plant desalination, sistèm subsea, ak anviwònman agresif pwosesis chimik.

 

Ki sa ki se 1.4462 materyèl?

1 . 4462, tou deziyen kòm x2crnimon 22-5-3, se yon estanda duplex asye pur ak en ekivalan a nan uns S31803 / s32205 (duplex 2205) . li gen ladan sou 22% Chromium, 5% corres, ak NOSTOM, ak NANSE ANTENSE ANTODOS ANDE ANDE ANDE ANTOME ANDE ANTOME ANDE ANTEN NAN NAN NAN 22. rezistans. Pandan ke yo pa klase kòm "super duplex," 1.4462 materyèl ofri pèfòmans ekselan nan anviwònman modera agresif, tankou tretman dlo ize, tank chimik, echanjeur chalè, ak kaka & papye sistèm-nan yon pri plis ékonomi konpare ak 1.4410.

 

1.4462 vs 1.4410 asye pur

 

1.4462 vs 1.4410 konpozisyon chimik (%)

Eleman 1.4462 / s32205 (duplex 2205) 1.4410 / s32750 (super duplex 2507)
CHROMIUM (CR) 21.0 – 23.0 24.0 – 26.0
Nikèl (Ni) 4.5 – 6.5 6.0 – 8.0
Molibden (MO) 2.5 – 3.5 3.0 – 5.0
Azòt (N) 0.14 – 0.20 0.24 – 0.32
Manganèz (MN) Mwens pase oswa egal a 2.0 Mwens pase oswa egal a 1.2
Silisyòm (SI) Mwens pase oswa egal a 1.0 Mwens pase oswa egal a 0.8
Kabòn (C) Mwens pase oswa egal a 0.03 Mwens pase oswa egal a 0.03
Fosfò (P) Mwens pase oswa egal a 0.03 Mwens pase oswa egal a 0.035
Souf (yo) Mwens pase oswa egal a 0.02 Mwens pase oswa egal a 0.02

 

duplex 2205 vs super duplex 2507 pwopriyete mekanik (nan tanperati chanm)

Posesyon 1.4462 / duplex 2205 1.4410 / super duplex 2507
Fòs rupture (MPa) 620 – 880 750 – 1000
Sede fòs (MPa) Pi gran pase oswa egal a 450 Pi gran pase oswa egal a 550
Elongasyon (%) Pi gran pase oswa egal a 25 Pi gran pase oswa egal a 15
Dite (HB) Mwens pase oswa egal a 290 Mwens pase oswa egal a 310
Enpak andirans Pi gran pase oswa egal a 100 j (nan -46 degre) Pi gran pase oswa egal a 80 j (nan -46 degre)

 

Pwopriyete fizik

Posesyon 1.4462 / duplex 2205 1.4410 / super duplex 2507
Dansite (g/cm³) 7.80 7.85
Modil Elastisite (GPA) ~200 ~200
Tèmik konduktivite (w/m · k) 19.0 14.0
Rezistivite elektrik (μω · m) 0.8 0.92
Koyefisyan ekspansyon (20-100 degre) (× 10⁻⁶/k) 13.0 12.5

 

1.4462 Chalè Tretman & Processing

Kalite tretman chalè 1.4462 / duplex 2205 1.4410 / super duplex 2507
Solisyon rkwir temp 1020 - 1100 degre 1050 - 1120 degre

 

 

Ka etid: duplex vs . super duplex nan dlo lanmè sistèm refwadisman

Yon izin elektrik Mwayen Oryan bezwen korozyon ki reziste kanalizasyon pou yonsistèm dlo lanmè refwadisman. Gnee okòmansman pwopoze1.4462 Duplex asye pur, men akòz segondè Salinity ak tanperati a, ekip la jeni chanje a1.4410 super duplex. laS32750 tiyoBay pi wo rezistans nan opozisyon ak estrès fann korozyon, asire operasyon ki an sekirite ak antretyen redwi sou yon 20- ane lifecycle . switch sa a ogmante pri materyèl inicio pa 18% men sove plis pase $ 300, 000 nan domaj potansyèl korozyon .}}}

1.4410 Super Duplex Stainless Steel Pipe

 

1.4410  Stainless Steel Pipe

 

Steel Gnee se yon dirijan din 1 . 4462 Nerjaveèi tiyo tiyo, distribitè ak founisè nan Lachin . Avèk plis pase 15 ane eksperyans nan, nou gen yon konpreyansyon gwo twou san fon nan endistri a asye ak gen anpil eksperyans kap bay gwo endistri yo.
Isit la yo se avantaj ki genyen nan chwazi asye goudwon:

✔ Ranje konplè nan klas duplex: 1.4462, 1.4410, S31803, S32750

✔ sètifye nan en 10216-5, ASTM A790, ISO 15156 (NACE)

✔ Dimansyon tiyo koutim, ekipman, ak sèvis fabwikasyon

✔ Sètifika tès moulen & enspeksyon twazyèm pati (BV, SGS, DNV)

✔ Sistèm enspeksyon pi byen - 100% tès NDT, tès pwopriyete mekanik, tès MPI

KontakGnee asye purpou1.4462 tiyo asye pursolisyon pwepare a pwojè ou .

Kontakte kounye a

1.4462 Stainless Steel Pipe
1.4462 tiyo asye pur
1.4410 Super Duplex Stainless Steel Pipe
1.4410 super duplex pur tiyo asye

Voye rechèch