1.4420 S31655 Nerjaveèi asye manifakti ak founisè

Jan 14, 2026

Kite yon mesaj

316L vs 904L Austenitic Stainless Steels: Standard Marine-Grade vs Strong Acid Resistance316H Stainless Steel High-CarbonASTM 201 Stainless Steel: Properties, Applications, and Limitations

Balans chimik 1.4420 S31655 estrikteman kontwole pandan pwosesis SMELTING nou an pou asire pèfòmans optimal. Anplis de sa nan Azòt se kle nan pwopriyete amelyore mekanik li yo.

Klas C (kabòn) Si (Silisyòm) Mn (Manganèz) P (fosfò) S (souf) Cr (Kwòm) Ni (Nikèl) Mo (Molybdène) N (Azòt)
1.4420 / S31655 Mwens pase oswa egal a 0.030% Mwens pase oswa egal a 1.00% Mwens pase oswa egal a 2.00% Mwens pase oswa egal a 0.045% Mwens pase oswa egal a 0.015% 16.5 – 18.5% 10.5 – 13.5% 2.0 – 3.0% 0.12 – 0.22%

 

 

1.4420 S31655 montre pi wo fòs sede pase asye pur austenitic konvansyonèl akòz ranfòse solisyon solid soti nan Azòt. Anba a se pwopriyete tipik nan tanperati chanm.

Pwopriyete Valè (tipik) Inite
Fòs rupture (Rm) 600 – 850 MPa
Fòs Sede (Rp0.2) Pi gran pase oswa egal a 290 MPa
elongasyon (A5) Pi gran pase oswa egal a 40 %
Dite (HB) Mwens pase oswa egal a 215 HB

 

Si ou gen kondisyon pwojè pou 1.4420 asye pur, nou akeyi lòd ou a. GNEE gen yon gwo envantè de pwodwi popilè pou ou pou w chwazi. Li ka trete nan divès fòm pwodwi pratik, ki gen ladan plak, bobin, tib, ba, fil, elatriye Pou enfòmasyon detaye sou konpozisyon chimik ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan. Imèl: info@gneestainless.com

 

Tès ak Dokimantasyon: Sètifika tès faktori, EN 10204 3.1, rapò chimik, rapò mekanik, rapò tès destriktif, rapò tès ki pa-destriktif, rapò tès PMI, rapò enspeksyon vizyèl, rapò enspeksyon twazyèm pati, rapò laboratwa sètifye NABL.
Anbalaj: anbalaj kès an bwa, anbalaj vlope jarèt, strapping asye, oswa anbalaj selon kondisyon kliyan.

Voye rechèch