Estanda ak Klas Ekivalan

 

UNS EN ASTM DIN GOST GB

SUS420J2

1.4034

Kalite 420 (Segondè-C)

X46Cr13

40Х13

4Cr13

 

 

Konpozisyon chimik

 

Klas Estanda C Kr Ni Mn Si P S Fe

420J2

JIS G 4303

0.26–0.40

12.0–14.0

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 0.04

Mwens pase oswa egal a 0.03

Balans

1.4034

EN 10088-2

0.43–0.50

12.5–14.5

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 0.04

Mwens pase oswa egal a 0.03

Balans

4Cr13

GB/T 1220

0.36–0.45

12.5–14.5

-

-

Mwens pase oswa egal a 1.0

Mwens pase oswa egal a 0.04

Mwens pase oswa egal a 0.03

Balans

 

 

Pwopriyete mekanik nan 420J2

 

Klas Estanda Fòs rupture Sede fòs Elongasyon Dite (Brinell)

SUS420J2

JIS G 4303

Pi gran pase oswa egal a 740 MPa

Pi gran pase oswa egal a 300 MPa

Pi gran pase oswa egal a 15%

Mwens pase oswa egal a 217 HBW (annealed)

1.4034

EN 10088-2

Pi gran pase oswa egal a 750 MPa

Pi gran pase oswa egal a 300 MPa

Pi gran pase oswa egal a 12%

Mwens pase oswa egal a 217 HBW

4Cr13

GB/T 1220

Pi gran pase oswa egal a 750 MPa

Pi gran pase oswa egal a 300 MPa

Pi gran pase oswa egal a 12%

Mwens pase oswa egal a 217 HBW