AISI 304 316 Bouton asye pur-soude tiyo Fittings Founisè

Jan 21, 2026

Kite yon mesaj

GNEE se yon manifakti pwofesyonèl ak ekspòtatè ekipman tiyo.
Pwodwi nou yo sitou gen ladan:
1) Nerjaveèi asye -fitting tiyo soude (koude,
diminye / egal tees, redukteur inik / konsantrik, bouchon tiyo, viraj, kwa, viraj retounen),
fabrike entèdi selon ASME/ANSI B16.9/16.28,
DIN 2605/2615/2616/2617, ak estanda EN10253.
2) Bride: konfòme ak ASTM / DIN / JIS / BS / EN ak lòt estanda.
Pwodwi nou yo sètifye PED ak ISO 9001.

AISI 304 316 stainless steel butt-welded pipe fittings
AISI 304 316 asye pur bout-soude tiyo fittings
AISI 304L stainless steel butt-welded pipe fittings
AISI 304L asye pur bou -soude tiyo ekipman

ASTM A403 WP 316 Tablo spesifikasyon koud tiyo

Espesifikasyon ASTM A403 / ASME SA403
Gwosè 1/8" NB POU 48" NB. (San pwoblèm ak 100% X-Ray soude, fabrike)
Estanda ASME/ANSI B16.9, ASME B16.28, MSS-SP-43
Epesè 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS ki disponib ak NACE MR 01-75
Kalite San pwoblèm / soude / fabrike

 

Gwosè 310 Nerjaveèi asye Buttweld Fittings

Gwosè: 1/8'' pou 104'', SCH5S ~ SCH160

Fen Koneksyon: Bou-soude.

Pwodwi Gwosè* Epesè miray la** San pwoblèm Soude
Koud 1/2"-24" SCH10S ~ XXS
8"-104" SCH5S ~ 80S/XS  
Tee 1/2"-24" SCH10S ~ XXS
8"-104" SCH5S ~ 80S/XS  
Larsen 1/2"-24" SCH10S ~ XXS
8"-104" SCH5S ~ 80S/XS  
Cap 1/2"-80" SCH10S ~ SCH160  
Lap Joint Stub Fen 1/2"-24" SCH5S ~ 80S/XS
8"-80" SCH5S ~ 80S/XS  

 

UNS S31600 Steel Reducer Chimik Konpozisyon Creole

Klas C Mn Si P S Kr Mo Ni N
316 min. 16.0 2.0-3.0 10.0
max. 0.035 2.0 0.75 0.045 0.030 18.0 14.0
316L min. 16.0 2.0-3.0 10.0
max. 0.035 2.0 0.75 0.045 0.030 18.0 14.0

 

ASTM A403 F316 Nerjaveèi asye egal Tee mekanik fòs

Klas Fòs rupture (MPa) min Sede fòs 0.2% Prèv (MPa) min Elongasyon (% nan 50mm) min Dite
Rockwell B (HR B) max Brinell (HB) max
316 515 205 40 95 217
316L 485 170 40 95 217