diferans ant 1.4404 ak 1.4432

Aug 26, 2025

Kite yon mesaj

Lè w ap chwazi asye pur pou pwojè ou yo, konprann diferans ki genyen ant 1.4404 (316L) ak 1.4432 se esansyèl. Tou de klas yo fè pati nan fanmi an asye pur austenitik ak yo trè rezistan a korozyon, men yo gen diferans kle nan konpozisyon chimik, pwopriyete mekanik, ak aplikasyon pou.

 

Ki sa ki 1.4404 asye pur?

1.4404 asye pur, ke yo rele tou 316L asye pur, se yon asye austenitik pur ak rezistans eksepsyonèl korozyon akòz kontni segondè li yo, nikèl, ak molibdèn. Kontni kabòn ki ba li yo (<0.03%) improves resistance to intergranular corrosion (sensitization) during welding, making it suitable for the manufacture of thick-gauge welded components. It can be processed into a variety of practical product forms, including sheet, coil, tube, bar, and wire. For detailed chemical composition and free samples, please contact us today.

 

Ki materyèl ki 1.4432 ekivalan a?

1.4436, 1.4435, ak 1.4432 materyèl yo pi bon ak ekivalan plis rafine nan asye 316L austenitik. Diferans debaz ki genyen ant klas yo se konsantrasyon nan aditif alyaj - nikèl, molibden, ak CHROMIUM.

 

Ki diferans ki genyen ant 1.4404 ak 1.4432?
EN 1.4404 ak 1.4432/1.4436 gen yon rezistans korozyon versatile epi yo apwopriye pou yon pakèt aplikasyon. Klas yo ki gen pi wo kontni molibdeni (1.4432,1.4436) te yon ti jan ranfòse rezistans korozyon konpare ak klas ki gen pi ba kontni molibdeni (1.4404).

Estanda

Estanda Deziyasyon
EN 10028-7, PED 2014/68/EU

1.4432

EN 10088-2

1.4432

EN 10088-3

1.4432; 1.4435

EN 10088-4

1.4432

 

Diferans ant 1.4404 ak 1.4432: konpozisyon

Posesyon 1.4404 (316L) 1.4432
CHROMIUM (CR) 16.5 – 18.5% 17.0 – 19.0%
Nikèl (Ni) 10.0 – 14.0% 9.0 – 12.0%
Molibden (MO) 2.0 – 3.0% 2.0 – 2.5%
Kabòn (C) Mwens pase oswa egal a 0.03% Mwens pase oswa egal a 0.03%
Manganèz (MN) Mwens pase oswa egal a 2.0% Mwens pase oswa egal a 2.0%
Fòs rupture 500-700 MPa 500-700 MPa
Sede fòs Pi gran pase oswa egal a 200 MPa Pi gran pase oswa egal a 200 MPa
Elongasyon Pi gran pase oswa egal a 40% Pi gran pase oswa egal a 35%

 

Èske 1.4404 plis rezistan a korozyon pase 1.4432?
Wi, 1.4404 (316L) gen yon kontni nikèl ki pi wo ak pi bon rezistans nan klorid, fè li pi apwopriye pou anviwònman maren ak trè korozivite.

 

Ki gen pi wo fòs, 1.4404 oswa 1.4432?
Tou de gen menm pwopriyete fòs (fòs rupture ~ 500-700 MPa), men 1.4404 se souvan pi pito pou aplikasyon pou maren ak chimik.

 

Ki pi bon pou pwosesis manje, 1.4404 oswa 1.4432?

Pou endistri a pwosesis manje, 1.4432 (AISI 316L) se souvan pi pito sou 1.4404. Kontni an ak anpil atansyon kontwole kabòn ki ba nan 1.4432 plis diminye risk pou yo kowozyon entèrgranilè, patikilyèman nan soud oswa chalè - zòn ki afekte yo, fè li pi apwopriye pou itilize nan ekipman konplèks pwosesis manje tankou tiyo, tank, ak veso depo. Esansyèlman, pandan ke tou de se manje - klas, 1.4432 ofri pwoteksyon ranfòse kont risk korozyon nan mande aplikasyon pou endistri manje.

 

1.4404 stainless steel

Ki moun ki chwazi nou?

 

Si ou gen yon bezwen pwojè pou 1.4404 asye pur, nou akeyi lòd ou yo. Gnee kenbe yon gwo envantè nan pwodwi popilè pou ou pou w chwazi nan. Nou travay sou pwodwi sa yo nan yon varyete de fòm pwodwi pratik, ki gen ladan fèy, bobin, tib, ba, ak fil. Pou konpozisyon chimik detaye ak echantiyon gratis, tanpri kontakte faktori nou an jodi a. Nou ofri prix konpetitif ak sèvis ekselan. Imèl:sales@gneestainless.com
 