ASTM A276 304/316L Nerjaveèi asye wonn sifas klere

Mar 16, 2026

Kite yon mesaj

What is 1.4460 Stainless Steel?What is the Equivalent of 1.4401 ?1.4122 material equivalent

Estanda

ASTM A276, ASTM A479/A479M, ASTM A484/A484M, ISO 683-13

Klas

00Cr17Ni14Mo2, 0Cr18Ni12Mo2Ti, 1.4404, SUS316L, X2CrNiMo17-12-2

Longè

Customized

Dyamèt

3 milimèt pou 500 milimèt (0.12-19.7 an), personnalisé

Fòm

Angle Bar, Channel Bar, Customized, Flat, Egzagonal, Rektangilè, Wonn, Kare, T-Bar

Sifas fini

2B, BA, nwa, bwose, Customized, kale, poli

Teknik

Fwad trase, frèt woule, cho woule

Fòm

Bar nan divès fòm, Fwad-Ba fini, Customized, Plat Bar, Fòje Bar, Hollow Bar, Cho-Roule Bar, Rod, Round Bar, Threaded Bar

 

Konpozisyon chimik

Kabòn (C) Silisyòm (Si) Manganèz (Mn) Fosfò (P) Souf (S) Kwòm (Cr) Nikèl (Ni) Molybdène (Mo) Azòt (N)
                 
Mwens pase oswa egal a 0.03 Mwens pase oswa egal a 0.75 Mwens pase oswa egal a 2.00 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.030 16.0 – 18.0 10.0 – 14.0 2.0 – 3.0 Mwens pase oswa egal a 0.10

Pwopriyete mekanik

Pwopriyete Inite metrik Inite Imperial
     
Fòs rupture 485 - 620 MPa 70 - 90 ksi
Sede fòs 170 - 310 MPa 25 – 45 ksi
Vickers dite 150 - 200 HV 150 - 200 HV
Brinell dite 146 – 217 HB 146 – 217 HB
Rockwell dite B80 – C20 B80 – C20
Elongasyon 40% – 50% 40% – 50%
Modil elastik 193 - 200 GPa 28 – 29 x 10^6 psi