ASTM A213 TP316L se yon varyant ultra-ki ba kabòn nan TP316, ki entegre molybdène-ki gen rezistans korozyon ak ultra-ki ba kabòn anti-intergranular kowozyon pèfòmans. Li fèt espesyalman pou soude-tib echanjeur chalè entansif ak tiyo pwosesis korozif ki piman bouk.
Klas ekivalan (orizontal)
UNS: S31603|JIS: SUS316L|GB: 022Cr17Ni12Mo2|EN: X2CrNiMo17-12-2|W.Nr.: 1.4404
Konpozisyon chimik (pwès%, orizontal)
C: Mwens pase oswa egal a 0.03|Si: Mwens pase oswa egal a 1.00|Mn: Mwens pase oswa egal a 2.00|P: Mwens pase oswa egal a 0.045|S: Mwens pase oswa egal a 0.030|Cr: 16.00-18.00|Ni: 10.00-14.00|Mo: 2.00-3.00|Fe: Balans
Pwopriyete kle (20 degre, rkwit, orizontal)
Dansite: 7.98g/cm³|Pwen k ap fonn: 1375-1450 degre|Fòs rupture: 485-650N/mm²|Sede fòs: Pi gran pase oswa egal a 170N/mm²|Elongasyon: Pi gran pase oswa egal a 40%|Dite: Mwens pase oswa egal a 217HB
Karakteristik debaz yo
• Ekselan pòs-soude rezistans korozyon entègranulèr, pa bezwen tretman pòs-soude recuit, anpil amelyore efikasite konstriksyon • Bonjan rezistans nan klori, asid ak medya alkali, apwopriye pou pwodui chimik, pharmaceutique ak anviwònman marin korozivite • Bon -tanperati severite, ka itilize san yo pa ka zo kase tanperati ki ba; pi ba fòs rupture pase TP316, men pi apwopriye pou soude - estrikti entansif
TP316 vs TP316L (Orizontal)
Kontni Kabòn: 316 (mwens pase oswa egal a 0.08%)|316L (mwens pase oswa egal a 0.03%)|Fòs rupture: 316 (515-690N/mm²)|316L (485-650N/mm²)|Apre-soude Recuit: 316 (Ka bezwen)|316L (Pa nesesè)|Kowozyon rezistans: 316 (Bon)|316L (ekselan)
| Klas | C | Mn | Si | P | S | Kr | Mo | Ni | N | |
| 316 | Min | - | - | - | 0 | - | 16.0 | 2.00 | 10.0 | - |
| Max | 0.08 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 | |
| 316L | Min | - | - | - | - | - | 16.0 | 2.00 | 10.0 | - |
| Max | 0.03 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | 0.10 | |
| 316H | Min | 0.04 | 0.04 | 0 | - | - | 16.0 | 2.00 | 10.0 | - |
| max | 0.10 | 0.10 | 0.75 | 0.045 | 0.03 | 18.0 | 3.00 | 14.0 | - |
Founisè asye pur
Si ou gen kondisyon pwojè pou asye pur, nou akeyi lòd ou a. GNEE gen yon gwo envantè de pwodwi popilè pou ou pou w chwazi. Li ka trete nan divès fòm pwodwi pratik, ki gen ladan plak, bobin, tib, ba, fil, elatriye Pou enfòmasyon detaye sou konpozisyon chimik ak echantiyon gratis, tanpri kontakte faktori nou imedyatman. Nou ofri pri konpetitif ak sèvis ekselan. Imèl: info@gneestainless.com



Tès ak Dokimantasyon: Sètifika tès faktori, EN 10204 3.1, rapò chimik, rapò mekanik, rapò tès destriktif, rapò tès ki pa-destriktif, rapò tès PMI, rapò enspeksyon vizyèl, rapò enspeksyon twazyèm pati, rapò laboratwa sètifye NABL.
Anbalaj: anbalaj kès an bwa, anbalaj vlope jarèt, strapping asye, oswa anbalaj selon kondisyon kliyan.


Voye rechèch