Avèk 18 ane eksperyans nan fabrikasyon tiyo, GNEE se yon founisè tiyo asye pur fè konfyans. Faktori nou an pa sèlman pwodui tiyo rkwit nan gwosè estanda, men li ofri tou tiyo ki pwolonje -longè 18 mèt ak 25 mèt pou satisfè bezwen kliyan divès kalite. Etablisman an konplètman ekipe, ki gen ladan moulen woule frèt, founo san lafimen, tank plonje, ultrasons ak machin netwayaj kouran eddy, osi byen ke laboratwa fizik ak chimik.

ASTM A269 Nerjaveèi Tubing Spesifikasyon
Non pwodwi: Tib asye pur ASTM A269
Kalite:Tib trase frèt san pwoblèm, tiyo san pwoblèm fini cho, tiyo soude, tiyo fabrike
Klas:ASTM A269 TP304, TP304L, TP304H, TP321H, TP321, TP316, TP316L, TP316Ti, TP310S, TP347, TP347H
Gwosè:1/8" NB a 24" NB, 1/4" OD a 24" OD gwosè asye pur tib san pwoblèm disponib tou
Longè:Jiska 6 mèt, longè koupe koutim
Epesè:1mm a 20mm, SCH 5/5S, 10/10S, 20/20S, 40/40S, 80/80S, 120/120S, 160/160S dapre ANSI B36.19/36.10
Fini:No.1 Pickled Fini, No.4 fini, BA Fini, Electropolished tiyo san pwoblèm
Konpozisyon chimik ASTM A269 TP304
| Klas | Ni | Kr | Mn | C | Si | S | P | |
| TP304 | Min | 8.0 | 18.0 | |||||
| Max | 12.0 | 20.0 | 2.00 | 0.08 | 1.00 |
0.03 |
0.045 |
ASTM A269 Gr TP304 Tib soude fòs mekanik
| Dansite | 8.0 g/cm3 |
| Pwen k ap fonn | 1400 degre (2550 degre F) |
| Fòs rupture | Psi - 75000, MPa - 515 |
| Fòs Sede (0.2% Offset) | Psi - 30000, MPa - 205 |
| Elongasyon | 35 % |
Karakteristik Fizik ASTM A269 304 Tib
| Klas | Dansite (kg/m3) | Modil elastik (GPa) | Mwayèn koyefisyan ekspansyon tèmik (m/m/0C) | Kondiktivite tèmik (W/mK) | Espesifik Chalè 0-1000C (J/kg.K) | Rezistans elektrik (nm) | |||
|---|---|---|---|---|---|---|---|---|---|
| 0-1000C | 0-3150C | 0-5380C | nan 1000C | nan 5000C | |||||
| 304 | 8000 | 193 | 17.2 | 17.8 | 18.4 | 16.2 | 21.5 | 500 | 720 |
ASTM A269 TP304 Lis pri tiyo
| Pwodwi | Pri |
|---|---|
| ASTM A269 TP304L 1" 2" 3" 4" 5" 6" x Sch 40 tib | $2.50 - $7.30/ Kilogram |
| 2 pous sch10s BE ASTM A269 SS304 Tiyo | $190.00 - $350.00/ pyès |
| Instrumentation Tib san pwoblèm ASTM A269 Bright Anneal marinated Nerjaveèi 304L 1/4,3/8,1/2,3/4 1 pous | $2.70 - $9.60/Mèt |
| ASTM A269 304 SS Tib san pwoblèm | $2.00 - $28.00/ Kilogram |
Nan GNEE, nou ofri pi bon pri sou ASTM A269 TP 304 asye pur tiyo san pwoblèm. Anpil founisè, grossistes, détaillants, distribitè, ekspòtatè, aksyonè, revandè, ak enpòtatè ASTM A269 304 tiyo asye pur ka jwenn gwosè yo bezwen nan envantè tiyo ASME SA269 TP304 nou an. Kontakte nou jodi a pou yon quote rapid! Imèl:sales@gneestainless.com
Sèvis nou yo
* Anbalaj: pake Bare, ranfòse ak espageti asye transverse. Pwa pake: 7-18 tòn
* Kantite: Customized bay lòd
* Marking: Pentire mak oswa etikèt / avek stickers son sou tèt pakèt yo, ki endike enfòmasyon yo mande yo.
* Tès: analiz konpozisyon chimik, tès tensile, tès plat, tès enpak, tès sele, enspeksyon dimansyon, enspeksyon vizyèl.
* Sètifika Tès: Sètifika tès faktori, rapò enspeksyon twazyèm -pati, ak sètifika matyè premyè
* Tan livrezon: atik nan-estok yo voye imedyatman; pwodwi Customized gen yon tan livrezon nan 15-30 jou.
* Valè-sèvis ajoute: Pre-tretman, koupe pati, enspeksyon twazyèm-pati, sèvis echantiyon, tès ultrasons, ak enspeksyon dimansyon.