316 (1.4401) vs 316L (1.4404): Ki sa ki nan diferans lan?
Apr 24, 2025
Kite yon mesaj
Diferans prensipal la antAISI 316 (1.4401) asye purak AISI 316L (1.4404) asye pur se kontni an kabòn. "L" la vle di pou kontni "ba kabòn". Akòz kontni an pi ba kabòn, AISI 316L (1.4404) Nerjaveèi asye gen yon risk redwi nan sansibilizasyon (grenn limit limit carbure presipitasyon), men an menm tan an pèdi kèk fòs. AISI 316LN (1.4406) se asye pur alye ak nitwojèn pou konpanse pou pèt la fòs.

Nòm AISI 316 \/ 316L \/ 316LN asye pur
| Rejyon \/ peyi | AISI 316 | AISI 316L | Aisi 316ln |
|---|---|---|---|
| USA (ASTM \/ AISI) | AISI 316, ASTM A240 \/ A276 \/ A479 | AISI 316L, ASTM A240 \/ A276 \/ F138 \/ A479 | AISI 316LN, ASTM A240 \/ A276 \/ A479 |
| Inyon Ewopeyen (EN \/ DIN) | EN 1.4401, x5crnimo 17-12-2 | EN 1.4404, x2crnimo 17-12-2 | EN 1.4406, x2crnimon 17-11-2 |
| Almay (DIN) | W.-Nr. 1.4401 | W.-Nr. 1.4404 | W.-Nr. 1.4406 |
| Lachin (GB\/T) | 022Cr17NI12MO2 | 022Cr17NI12MO2 | 022Cr17NI12MO2N |
| Japon (JIS) | Sus 316 | Sus 316l | Sus 316ln |
| Larisi (GOST) | 03Х17Н13М2 | 03Х17Н13М2 | 03Х17Н12М2Н |
| ISO Creole | ISO 15510 x5crnimo 17-12-2 | ISO 15510 x2crnimo 17-12-2 | ISO 15510 x2crnimon 17-11-2 |
AISI 316 vs 316L vs 316LN Nerjaveèi asye konpozisyon chimik
| Eleman | AISI 316 (1.4401) | AISI 316L (1.4404) | AISI 316LN (1.4406) |
|---|---|---|---|
| Cr (CHROMIUM) | 16.5–18.5% | 16.5–18.5% | 16.5–18.5% |
| Ni (nikèl) | 10–13% | 10–13% | 10–12.5% |
| MN (Manganèz) | Mwens pase oswa egal a 2% | Mwens pase oswa egal a 2% | Mwens pase oswa egal a 2% |
| MO (MOLYBDENUM) | 2–2.5% | 2–2.5% | 2–2.5% |
| Si (Silisyòm) | Mwens pase oswa egal a 1% | Mwens pase oswa egal a 1% | Mwens pase oswa egal a 1% |
| N (nitwojèn) | 0.11% | 0.11% | 0.12–0.22% |
| P (fosfò) | Mwens pase oswa egal a 0. 045% | Mwens pase oswa egal a 0. 045% | Mwens pase oswa egal a 0. 045% |
| C (kabòn) | Mwens pase oswa egal a 0. 07% | Mwens pase oswa egal a 0. 03% | Mwens pase oswa egal a 0. 03% |
| S (souf) | 0.03% | 0.02% | 0.015% |
AISI 316 vs 316L vs 316LN karakteristik asye pur (valè tipik nan 20 degre)
| Posesyon | AISI 316 (1.4401) | AISI 316L (1.4404) | AISI 316LN (1.4406) |
|---|---|---|---|
| Densite | 8 g\/cm³ | 8 g\/cm³ | 8 g\/cm³ |
| Modil elastik | 193 GPA | 193 GPA | 200 GPA |
| Dite (Brinell) | Max 215 Hb | Max 215 Hb | Max 220 Hb |
| Fòs rupture | 500-700 MPa | 520–680 MPa | 580-780 MPa |
| Sede fòs | 200 MPa | 220 MPA | 205 MPa |
| Ekspansyon tèmik | 1.59 × 10⁻⁵ /K | 1.59 × 10⁻⁵ /K | 1.59 × 10⁻⁵ /K |
| Tèmik konduktivite | 16.3 W/(m·K) | 16.3 W/(m·K) | 15 W/(m·K) |
| Pwen k ap fonn | ~ 1400 degre | ~ 1400 degre | ~ 1400 degre |
Aplikasyon komen nan 316\/316L\/316LN asye pur
Estrikti Aerospace
Pr,
Ekipman pwosesis manje
Ekipman bwasri
Kaka ak ekipman papye
Petwòl ak petwòl ekipman raffinage
Resipyan transpò chimik
Savon ak foto ekipman pwosesis
Ekipman endistri tekstil
Achitekti
Ekipman pwosesis famasetik
Workbenches laboratwa ak ekipman
Pwodwi pou Telefòn maren
Echanjeur chalè
Voye rechèch