1.4438 / 317L / x2CRNIMO 18-15-4 Materyèl Fèy Done
Jun 13, 2025
Kite yon mesaj
1.4438 / 317l / x2crnimo 18-15-4. PDF
Ki materyèl ekivalan 1.4438 asye pur?
| Posesyon | Deskripsyon |
|---|---|
| En non estanda | 1.4438 |
| AISI/ASTM ekivalan | AISI 317L |
| DIN Deziyasyon | X2crnimo 18-15-4 |
| Nimewo uns | S31703 |
| Fòm pwodwi | Plak, fèy, tiyo, tib, ba, ekipman |
| Estanda | ASTM A240, A312, A213, EN 10088-1, ISO 15510 |
Ki konpozisyon chimik x2crnimo 18-15-4?
Konpare ak 316L, 317L gen plis nikèl ak molibdèn, ofri amelyore rezistans opoze .
| Eleman | Kontni (%) |
|---|---|
| Kabòn (C) | Mwens pase oswa egal a 0.030 |
| CHROMIUM (CR) | 18.0 – 20.0 |
| Nikèl (Ni) | 13.5 – 15.0 |
| Molibden (MO) | 3.0 – 4.0 |
| Manganèz (MN) | Mwens pase oswa egal a 2.00 |
| Silisyòm (SI) | Mwens pase oswa egal a 1.00 |
| Fosfò (P) | Mwens pase oswa egal a 0.045 |
| Souf (yo) | Mwens pase oswa egal a 0.015 |
| Azòt (N) | Mwens pase oswa egal a 0.10 |
| Iron (Fe) | Res |
Ki pwopriyete mekanik AISI 317L?
| Posesyon | Valè (tipik) |
|---|---|
| Fòs rupture (RM) | 540 - 750 MPa |
| Fòs sede (RP0.2) | Pi gran pase oswa egal a 240 MPa |
| Elongasyon (A5) | Pi gran pase oswa egal a 40% |
| Dite (HBW) | Mwens pase oswa egal a 220 |
| Modil Elastisite | ~ 200 GPA |
| Dansite | ~ 8.0 g/cm³ |
| Ranje k ap fonn | 1370-1395 degre |
Ki sa ki estanda a nan 1.4438 asye pur?
| Klas: | X2crnimo 18-15-4 | |||||||||
| Nimewo: | 1.4438 | |||||||||
| Klasifikasyon: | Austenitik asye pur - Klas Espesyal | |||||||||
| Dansite: | 8 g/cm ³ | |||||||||
| Creole: |
|
Ki valè pren 317L?
Pren (rezistans rezistans nimewo ekivalan):~33–35, pi wo pase 316L (~ 24-27)
Ki diferans ki genyen ant 1.4438 ak 316L?
Diferans prensipal ki genyen ant 1 . 4438 (317L) ak 316L (1.4404) asye pur manti nan kontni molibdèn ak nikèl yo, ki afekte dirèkteman rezistans korozyon yo.
1.4438 contains more molybdenum (3.0–4.0%) and nickel (13.5–15%) than 316L (Mo ~2.0–2.5%, Ni ~10–13%), giving it better resistance to pitting and crevice corrosion, especially in chloride-rich or acidic environments. Sa fè 317L plis apwopriye pou mande pwosesis chimik oswa aplikasyon pou maren, pandan y ap 316L se pi pito nan aplikasyon jeneral korozyon ki reziste ak pi ba pri.
📦 Fòm ekipman pou
Plak & Dra:Cho/frèt woule, 2b, pa gen .1, pa gen .4, Ba fini
Tiyo & tib:San pwoblèm & soude (ASTM A312 / A213)
Ba & baton:Wonn, kare, hex
Anwoulman & bann:Pou echanjeur chalè ak fabwikasyon tank
Fittings & Flanges:Pou sistèm tiyo presyon
Sètifika tès moulen (en 10204 3.1/3 . 2) Disponib sou demann.